Any of the SE Queensland members know if the foundry at Dalby is still operating?
I have a cast steel part to either fabricate or get cast.
The original is cracked from a major bingle with a bigger machine, and cant be safely repaired by welding as its a safety issue.
Fabrication will take a while as there is a quite a few machined surfaces and bores.
It is similar to the pivot assembly on a backhoe.
Michael
-
31st Jul 2016, 11:59 AM #2
Looking like I will have to either find a part from a machinery dismantler or spend big$ for a new part .
It seems that manufacturing in Australia is non existent , or people don't want to take on difficult tasks.
Michael
-
31st Jul 2016, 04:19 PM #3Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
Mike, what's the part you're looking for, someone on here may know of a part for you???
You're right about the manufacturing industry, it seems the Govt with its RED tape and unions, don't want it here????
KrynTo grow old is mandatory, growing up is optional.
-
31st Jul 2016, 06:18 PM #4Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,216
I take it Doug Slack foundry no longer exists?
Gold, the colour of choice for the discerning person.
-
31st Jul 2016, 07:59 PM #5
RC No they closed quite some time ago.
Whites in Dalby may be the closest and they will do small one off jobs .
The price from OEM is over $8k , it would take quite a long time to fabricate one and it would need stress relieving before machining as the welding will induce a lot of stress.
The machining would be about a week in between jobs , lots of bushes and bearing fits.
Casting would only require machining .
I am waiting for an email and then can decide if its worth continuing to get it cast.
Michael
Similar Threads
-
Antique cast iron clamp part fixed
By aametalmaster in forum METALWORK GENERALReplies: 2Last Post: 9th Sep 2013, 07:17 PM -
Cast iron VS Cast steel lathe compound slide
By Ueee in forum METALWORK GENERALReplies: 10Last Post: 23rd Dec 2012, 11:40 PM -
welding cast iron to steel
By Knotaclue in forum WELDINGReplies: 2Last Post: 8th Oct 2010, 10:11 PM -
Removing cast handwheel from steel shaft
By billrule in forum METALWORK GENERALReplies: 14Last Post: 10th Oct 2009, 08:24 PM -
can anyone weld cast steel?
By Aaron r in forum WELDINGReplies: 2Last Post: 29th Dec 2008, 12:01 AM