    Default Newcastle Furnace Material Suppliers

    I'm just starting my furnace build.
    Plan is castable 1600ºC hot face, kaowool insulation backing, waste oil burning (the brute style design).

    Hopefully someone else local finds this helpful
    I spent quite a while trying to find suppliers without much success until a business referred me on to:

    Beroa
    303/1B George St
    Mayfield NSW
    (02) 4960 0441

    I wandered in, and they are clearly set up for big jobs for industry, but they were extremely helpful. Michael assisted me and knew exactly what I needed.

    $50 even for a 25kg bag of Duracast 1600AR ($83 at Field Furnace Refractories).
    They also sell Kaowool, at about $100 for a roll of 50x610x3660 or 25x610x7320. I won't need nearly that much, so they advised me to pop in in a week or so, when they've finished a job, and they'll likely have some offcuts that I can buy.

    I was contemplating freight from Sydney for this stuff, so it was a great find.

    Now I just need to find a decent furnace shell.

  2. #2
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    From: http://www.engsupplies.com.au/dense-castables.html

    DURACAST 1600AR

    DESCRIPTION:

    A conventional cement bonded castable, which has good strengths and dimensional stability.

    Maximum Service Temperature (oC) 1600

    Dry material required per cubic metre (kg) 2140

    Maximum grain size (mm) 8

    Water addition (litre/100 kg) 10-12

    MODULUS OF RUPTURE (MPa)

    After drying at 110oC 12

    After heating to 1000oC 8

    After heating to 1600oC 12

    COLD CRUSHING STRENGTH (MPa)

    After drying at 110oC 50

    After heating to 1000oC 40

    After heating to 1200oC 90

    PERMANENT LINEAR CHANGE (%)

    After drying at 110oC neg

    After heating to 1600oC -1.5

    THERMAL CONDUCTIVITY (cast)

    At a mean of 1000oC (W/m/oK) 0.85

    Storage life (under ideal conditions) Twelve (12) months

    TYPICAL CHEMICAL ANALYSIS (%)

    Al2O3 SiO2 Fe2O3 CaO TiO2 Alkalies
    56 37 0.6 4.8 1.5 0.4

  3. #3
    Join Date
    Jan 2012
    Location
    Hinchinbrook
    Posts
    112

    Default

    Quote Originally Posted by pippin88 View Post
    I'm just starting my furnace build.......Now I just need to find a decent furnace shell.
    You dont say what size, but lpg cylinders make great shells.

    Cheers Phil

  4. #4
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Phil,

    I'd like a chamber size of 8-10". Planning 1" refractory, 2" ceramic wool.
    I've seen lpg tanks used as shells - just need to find one, not sure where they go to heaven?

  5. #5
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Manage to snag a 9kg LPG cylinder (well actually tetrafluoroethylene, which is non-flammable) at a scrap place today. They had a skip full of 9kg cylinders. Had some bigger ones too (45kg I guess).

    They gave it to me for free because they are not allowed to sell to the public...
    Very nice of them.

  6. #6
    Join Date
    Dec 2010
    Location
    Mornington Peninsula
    Posts
    97

    Default

    Any progress on the furnace build and how it is all coming together?

    Pictures would be great.

  7. #7
    Join Date
    Sep 2009
    Location
    Newcastle
    Posts
    342

    Default

    Haven't got any further, been working on other projects.

    Starting to plan again however, having been inspired by myfordboy on YouTube.

Similar Threads

  1. Small furnace
    By Woodwould in forum METALWORK GENERAL
    Replies: 5
    Last Post: 12th Jul 2010, 02:53 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •