Thanks Thanks:  0
Likes Likes:  0
Needs Pictures Needs Pictures:  0
Picture(s) thanks Picture(s) thanks:  0
Results 1 to 5 of 5

Thread: burner help

  1. #1
    Join Date
    May 2002
    Location
    in the outer reaches of Sth Oz
    Age
    75
    Posts
    525

    Default burner help

    In the morning I am purchasing the last bits for making my furnace but will need to find some place that has info on making the lpg burner. I will be melting aluminium so would like a natural aspirated burner. Any sites would be appreciated as when I google I get too many hits and would prefer links that you people like
    Pete
    Boycott Shampoo!!
    Demand Real Poo!

  2. #2
    Join Date
    Nov 2006
    Location
    Darwin HowardSprings
    Age
    52
    Posts
    41

    Default The site ive been on lately

    Burner engineering

    why propane ? its always hard to use up a bottle , and if you pull too much gas out too fast , they freeze over ?

    Diesel burner
    is my diesel burner , its good for aluminium with a #10A crucible , not enough air flow for copper alloys , so am about to make a new Waist Motor Oil burner for copper , well the above burner is running straight WMO at the moment test my new plans , and is melting copper
    how come a 10mm peg dont fit in a 10mm hole

  3. #3
    Join Date
    Nov 2006
    Location
    Darwin HowardSprings
    Age
    52
    Posts
    41

    Default

    if you do start too use that forum , they will expect you to have read this Foundry Tutorial Book

    just so you dont ask the same questions that were asked every 2 days before ^^^that page was written
    how come a 10mm peg dont fit in a 10mm hole

  4. #4
    Join Date
    May 2002
    Location
    in the outer reaches of Sth Oz
    Age
    75
    Posts
    525

    Default

    Thanks for that Mr Sniffer It would have taken me days or weeks to find that site. I'm starting with the furnace shown in this site and if I like what I do with it I may look at other metals for melting. For now small steps to get the experience.
    Pete
    Boycott Shampoo!!
    Demand Real Poo!

  5. #5
    Ueee's Avatar
    Ueee is offline Blacksmith, Cabinetmaker, Machinist, Messmaker
    Join Date
    Dec 2011
    Location
    Canberra
    Age
    40
    Posts
    4,515

    Default

    Good forum that. Lots of good info. I had a look at your post on your furnace Sawdust, looks like you are getting it working well.
    1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.

Similar Threads

  1. Forced Air LPG Burner Mk2
    By RayG in forum THE FOUNDRY
    Replies: 26
    Last Post: 6th Jun 2011, 12:50 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •