    Started with some 20x20mm square bar stock and had to upset the ends.

    Shaping the ends


    It’s very awkward to work these heavy and long bars on your own over the anvil. The mass allows a lot of absorbed heat down the length where you want to hold the bar and the length out back is trying to fight you whilst your trying to be accurate with the hammer blows on the end. I used a support stand on the end to some success.


    Had to do some research and test pieces for the square pass through. Lots of conjecture and and differing options on how to do this.


    Drew out my long tapers on all the bars.


    Slitting bars and they line up perfectly.


    Main structural components forged. Lots of holes!
    …..Live a Quiet Life & Work with your Hands

  2. #2
    Join Date
    Apr 2014
    Location
    Perth
    Posts
    134

    Default

    hi
    what are these for?
    steve

  3. #3
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    Steve, parts for a sculpture I’m making for the Lilydale Agricultural Show if it all works out.
    …..Live a Quiet Life & Work with your Hands

  4. #4
    Join Date
    Aug 2010
    Location
    Horsham Victoria
    Posts
    113

    Default

    I’m looking forward to seeing how this one develops.

    Looks good

  5. #5
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    …..Live a Quiet Life & Work with your Hands

  6. #6
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default



    …..Live a Quiet Life & Work with your Hands

  7. #7
    Join Date
    Apr 2014
    Location
    Perth
    Posts
    134

    Default

    nicely done dale how long did it take you
    steve

  8. #8
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    I should keep some sort of time sheet on these ‘things so I have an accurate account. I have been working on it for about a month on and off. I think I have about 6-7 Days in it.

    There is still more components to go on it the should be a scroll/ribbon and it will need some sort of base.
    …..Live a Quiet Life & Work with your Hands

  9. #9
    Join Date
    Apr 2013
    Location
    Canberra
    Posts
    54

    Default

    That is some lovely smithing, very accurate!! I’m impressed. I’ve been wanting to try some of these techniques for a while but there is never enough time for play when I have knife orders to work on!

    I know you said there was some conjecture, but what’s the thoughts behind slitting, rounding and then squaring, over punching and then drifting (like doing a hammer eye)?

  10. #10
    Join Date
    Dec 2007
    Location
    Melbourne
    Posts
    1,628

    Default

    It’s all about the way the metal moves. The thinnest part stretches the most becoming thinner still. So if you punch and drift you have less surface area and get a thinner wall on the drifted hole.

    when you slit you slit to the finished hole size. The length of the slit = finial perimeter/diameter. Of hole. So wall thickness stays even.

    drifting round is just a way of reshaping the slit evenly in transition to square. This is where it’s debated if it is needed. Some believe going straight to a square drift can catch on the corners and leave the sides thicker and stretch the metal thin at the top and bottom.

    i know what i´m trying to say, I hope it translates lol
    …..Live a Quiet Life & Work with your Hands

  11. #11
    Join Date
    Apr 2013
    Location
    Canberra
    Posts
    54

    Default

    Translated perfectly and it makes total sense. A good piece of info for when I get around to having a go, thank you

Similar Threads

  1. Your latest project
    By .RC. in forum METALWORK GENERAL
    Replies: 3019
    Last Post: 9th Apr 2024, 12:57 PM
  2. My latest TAD project
    By Michael G in forum METALWORK PROJECTS
    Replies: 2
    Last Post: 23rd Aug 2017, 08:52 AM
  3. your latest project
    By krisfarm in forum METALWORK GENERAL
    Replies: 9
    Last Post: 10th Feb 2012, 04:53 PM
  4. latest little project
    By wayno60 in forum WELDING
    Replies: 3
    Last Post: 12th Jul 2008, 03:40 PM
  5. Latest project WIP
    By Andy Mac in forum METALWORK GENERAL
    Replies: 5
    Last Post: 27th Jun 2007, 05:44 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •