Quote Originally Posted by Grahame Collins View Post
A very nice anvil Tuomas..

Thank you.
No, i didn't weld it all. I actually wanted to use angle grinder for making as much it was possible.

Making can be seen from this video, if one is interested?

https://youtu.be/Ysq9GlRPCMg

Here is one picture more about the door wreath.
Contrast between the rust and stainless can be seen from it. Picture is taken after couple weeks outsides, after years it becomes deeper. That door is under the roof, so it darkens very slowly, but some changes has happened. Originally it was brushed and little shiny.

FQ7VQKXIVO3TA2H.LARGE.jpg

I personally like to mix stainless materials to ferrite ones, can't say what makes it so tempting. I just like the contrast between them. 😊