Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 9 of 9
Thread: Anvils
-
19th Feb 2013, 09:26 AM #1New Member
- Join Date
- Nov 2012
- Location
- Tasmania
- Posts
- 1
Anvils
I notice that some one in Victoria is selling new 10kg anvils on ebay for $85, presumably Chinese. They have no hardy hole.
Does anyone have any knowlegde of these? Are they cast iron and likely to break?
Bob
-
19th Feb 2013, 01:04 PM #2Senior Member
- Join Date
- Dec 2009
- Location
- Sydney
- Posts
- 327
G'day Bob,
I reckon you would be better off taking your $85 to a metal yard and get a piece 2" thick x your fist-to-floor height, and make it stand up.
See; Brazeal Anvil Rising * 4" Plate Anvil (with pics) - Anvils - I Forge Iron
good luck,
AndrewOC'Waratah' spring hammer by Hands & Scott c.1911- 20, 'Duffy, Todd & Williams' spring hammer c.1920, Premo lathe- 1953, Premo filing machine.
-
19th Feb 2013, 02:00 PM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
If you are after something super cheap maybe take a look at the McJing anvils - at least they have a hardy hole.
11kg for $59, 33kg for 98 and 25 kg for $149, As usual freight is a problem but maybe get them to bring one down when the woodshow is on?
-
20th Feb 2013, 03:10 AM #4Senior Member
- Join Date
- Oct 2003
- Location
- Sydney,Australia
- Posts
- 174
Almost certainly cast iron of some sort, not suitable for pounding on. The large ones that were on sale a few decades ago, around 100lbs, were OK as tool holders or for setting rivets for leatherwork on, but cracked in half if used for forging. If they didn't crack in half then they were soft as old chewing gum and basically sagged into uselessness. Anything too small doesn't have the mass to stop it bouncing around, and no hardy hole means you can't fit any of the usual tools to it - its basically a boat anchor or decorator item.
Good anvils are not cheap, even second hand anvils that haven't been abused as hard to find, they have either been turned into scrap by unthinking or caring owners or have been snapped up by interior decorators......or people like US. 'Real' anvils are still being made, but freight is going to kill you.
-
20th Feb 2013, 10:38 AM #5New Member
- Join Date
- Nov 2012
- Location
- Tasmania
- Posts
- 1
Anvils
Thanks for the comments. In response to my question the seller advised that it was cast iron.
I won't waste my money, scrap steel is the way to go,
Bob
-
27th Feb 2013, 12:22 PM #6Member
- Join Date
- Feb 2013
- Location
- Picton NSW
- Posts
- 82
I recently picked up some old forklift tines from a dealer for next to nothing. They are great steel for an anvil, though the ones I got are a little thin... Probably I will use them for hammers and tools.
The point is though ask around and you will be amazed what you can get for very little cash.
-
27th Feb 2013, 02:06 PM #7Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
-
27th Feb 2013, 07:25 PM #8Member
- Join Date
- Feb 2013
- Location
- Picton NSW
- Posts
- 82
D'oh, They are normally good carbon steel, 4140 or better. They are normally forged and heat treated. they also come in monster sizes up to about 100mm thick for the real big ones. Definitely worth keeping an eye out for. If you find any and don't want them let me know I will take em if I can get em!
-
27th Feb 2013, 07:26 PM #9Member
- Join Date
- Nov 2007
- Location
- mid north coast NSW
- Posts
- 92
BobL, Have alook at this blokes forklift tine anvil. Lots of other interesting stuff here also!Fred Connell - Blacksmith
Graeme
Similar Threads
-
Anvils?
By Aerohydro in forum THE SMITHYReplies: 36Last Post: 11th Nov 2012, 11:16 PM -
Anvils for sale- SE Qld.
By Andy Mac in forum METALWORK GENERALReplies: 0Last Post: 25th Oct 2008, 12:45 PM -
Anvils
By Marc in forum METALWORK GENERALReplies: 2Last Post: 28th Sep 2007, 06:38 PM