What grade steel for cross/ compound screw
What is the preferred type/grade of steel for making cross/compound slide screws?
-
9th Aug 2018, 08:56 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
For easy thread cutting, some 1214 would be good but really just about grade of steel will do as lead screws are not highly stressed, are (or should be) well lubricated and have relatively low loads on them in respect to their size.
Michael
-
10th Aug 2018, 07:49 AM #3Most Valued Member
- Join Date
- Jul 2016
- Location
- Melbourne
- Age
- 35
- Posts
- 1,522
Like Michael said, anything you can get a good finish on really.
-
10th Aug 2018, 08:04 AM #4Pink 10EE owner
- Join Date
- Aug 2008
- Location
- near Rockhampton
- Posts
- 6,218
I made one out of 4140. In the US they can get a high carbon free machining steel, it would be ideal. It is 1144.
Gold, the colour of choice for the discerning person.
Similar Threads
-
Myford ML7 cross slide and compound screws
By dadrock in forum METALWORK GENERALReplies: 11Last Post: 14th Apr 2018, 11:48 AM -
260 Compound and Cross Slide Micrometer stud thread???
By ventureoverland in forum THE HERCUS AREAReplies: 4Last Post: 25th Nov 2014, 03:41 PM -
Removing a Sheraton compound feed screw
By coffeefro in forum METALWORK GENERALReplies: 8Last Post: 3rd Oct 2011, 09:42 PM -
Metric cross slide screw.
By pipeclay in forum THE HERCUS AREAReplies: 14Last Post: 20th May 2011, 11:59 PM -
cross feed screw
By azzrock in forum THE HERCUS AREAReplies: 57Last Post: 6th Feb 2011, 05:41 PM