Hey Kryn i cant find anyone who can bend or roll T6 alloy i beam
-
29th Jun 2018, 06:56 PM #17Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
What equipment do you have available? Asking, as it looks like you'll have to make a roller if these places can't do it.
https://www.yellowpages.com.au/nsw/w...nessTypeSearch
https://www.yellowpages.com.au/nsw/r...nessTypeSearch
https://www.yellowpages.com.au/nsw/p...nessTypeSearch
KrynTo grow old is mandatory, growing up is optional.
-
3rd Jul 2018, 01:05 AM #18Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Im going to try the original idea using the 100x50x4mm open channel beam, the beam will be open to the outside of the frame so i can weld some 50x50x3mm cross members
I firstly need to some how attach my multimeter to my welders terminals and video record my settings and write the down need to kick this trailer off by setting up the welder correctly from the beginning
-
10th Jul 2018, 11:54 PM #19Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
I have thought about making the roller that is a great idea and i have a plan in my head but it requires a lathe to machine the rollers, do any of u know of any cheap lathe deals around $400? I have looked at the Chinese mini lathes on ebay and made in china they start around $600
-
11th Jul 2018, 12:23 AM #20Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I'd stay away from any of the mini stuff, plastic gears etc. DAMHIKT.
You might be able to get a member to turn up the necessary bits for the roller, while saving/looking for a bigger/better lathe.
KrynTo grow old is mandatory, growing up is optional.
-
11th Jul 2018, 01:36 AM #21Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
I was looking at the 7x14 Chinese lathes unsure if they are ran by plastic, metal gears or belts 550watt motors, i tried looking for steel round bar in 100mm+ size couldn't find it for some reason for the rollers, do u think machine grade aluminum rollers would be ok?
i thought about sending an email to one of the machinist on Gumtree asking about making the rollers but as it is the 3x alloy rollers in 130mm are $150 plus the cost of paying someone to machine them would likely put the price up there i could add a little more to buy a machine and make multiple sets of all different sizes and forms
besides i have wanted a nice little hobby lathe for a while now just cannot manage to save enough tho, i tried searching Gumtree for a larger vintage model lathe but none available
-
11th Jul 2018, 11:54 PM #22Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
What are the rollers for? If they are for the keel to run on, I'd use the polyurethane type, they don't rust, corrode or give problems.
If the rollers are for something else, I might be able to get hold of some and bring it over next week for you. Let me know if you need it and I'll get a price for you?
KrynTo grow old is mandatory, growing up is optional.
-
12th Jul 2018, 03:04 AM #23Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Hey Kryn, the rollers are for the metal rolling device to roll the alloy i beam or U channel steel for the trailer frame
-
13th Jul 2018, 01:00 AM #24Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
I don't think the ally would hold up too long.
I'll get a price for you tomorrow. Will be leaving next Thursday, so I can bring it with me if the price is OK.
KrynTo grow old is mandatory, growing up is optional.
-
13th Jul 2018, 04:03 PM #25Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,916
I think you are seriously underestimating the force required to roll 100X50X4 steel channel (which I reckon is under specced for a trailer anyway). Have a look at the section rollers at machinery house https://www.machineryhouse.com.au/Se...h&s=section%20
These are substantial bits of gear, but even then, you need one of the larger models in order to roll channel like you are talking about.
If you are welding 50X50X3 in as cross members, why not bite the bullet and use RHS for the whole construction?
-
13th Jul 2018, 05:02 PM #26Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Karl i dont have a lot of cash trying to make the most of what i have and what i can save in the future, the shs cross members were one option what i am trying to do well hopefully is buy pre galvanized steel so i only need to coat the welds with lanolin, i was quoted for the trailer to be galvanized $5 per killo thats a whopper when your talking 150-200kg frame plus i will need to haul the frame 5 hours north and hire a car trailer for total 10 hours on 2 occassions it all adds up financially, i do have a trailer now that my boats on but i would need to cut out sections as it has splits and rust
-
13th Jul 2018, 07:20 PM #27Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,229
Wouldn't the price for galvanizing be per kg of galv they put on not what the trailer actually weighs? Pretty sure that's how we get charged at work.
-
13th Jul 2018, 07:37 PM #28Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Ah ok i misunderstood how it was priced and weighed, what would a 5.5 meter boat trailer cost to gal?
-
14th Jul 2018, 11:23 PM #29Senior Member
- Join Date
- Oct 2015
- Location
- melbourne
- Posts
- 473
I've always wondered about gal costs, I have some old H beam I'd like to use for low retaining walls.
According to Industrial Galvanizers - SPECIFIERS MANUAL
It is charged by the weight of the item. The rate may vary with the type of item, thin /complex items are dearer than larger thick items.
But that link suggests $5/kg may be a bit on the high side.
Russ
-
14th Jul 2018, 11:28 PM #30Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Ok here's a curve ball i tried googling this last night, how much is 1kg of zinc in litres or how many square meters would 1kg cover? i just don't want to built a trailer haul it to the galvanizer have the job dipped than they charge triple or more than what i expected
Similar Threads
-
Beam deflection
By Gestalt in forum METALWORK GENERALReplies: 32Last Post: 25th Nov 2017, 07:11 PM -
Beam Deflection and Stress Calculator
By KBs PensNmore in forum CONVERSIONS & CALCULATIONSReplies: 0Last Post: 20th Nov 2017, 06:40 PM -
Making a Steel Beam Flat
By grunto in forum METALWORK GENERALReplies: 15Last Post: 26th Jun 2017, 09:31 PM -
Building a Aluminium I Beam Trailer
By gazza2009au in forum TRAILERS & OTHER FABRICATED STUFFReplies: 58Last Post: 30th Mar 2015, 11:45 PM -
Cornish beam engine
By neksmerj in forum METALWORK GENERALReplies: 5Last Post: 22nd Aug 2013, 01:05 PM