Extending trailer stub axles?
Hi all,
I'm in the process of building an hydraulic log splitter and I'm at the stage of attaching the axles to the frame. To keep the design as simple as possible, I have opted not to have any suspension and will weld the axles to the frame at a pre-determined point where there is a cross member. I estimate that the finished splitter will be around the 600Kg mark and with the wheels in this position should provide me with a ball weight of about 60 - 65Kg. The supporting trailer frame is based loosely on a 5x3 trailer but with a slightly longer drawbar in order to house the 1.6L corolla motor and it's radiator.
The frame is made from 100x50x3mm RHS.
For the axles, I have a couple of re-purposed stub axles that are 200mm long. Thye came off another trailer that has since been scrapped but it would be a shame to not use some of the parts such as the wheels, hitch etc. Only issue is these stub axles came from a home made independent susppenson and are not long enough for my use. Ideally, I would like to make them a single axle by a legitimate joining method. Bare in mind that if they are joined, the joint will end up roughly where the axle extends past the trailer frame.
Can these two axles be safely joined by housing inside a piece of substantial square tube of sufficient wall thickness, using decent welds? 20180223_215221.jpg
Any suggestions or advice is much appreciated.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
23rd Feb 2018, 10:51 PM #2Novice
- Join Date
- Mar 2016
- Location
- Sutherland Shire, Sydney
- Posts
- 24
Might have missed something Simone but if you are going to tow this at more than say 20kmh and or on the road etc then Id put a set of springs under it, less shock on everything, longer life etc, cant answer the question on joining the axels, prob just easier to buy an axle that matches your hubs,
-
23rd Feb 2018, 11:30 PM #3Intermediate Member
- Join Date
- Feb 2018
- Location
- Loxton
- Age
- 54
- Posts
- 37
Legalities aside as I am not sure of those, sure you can extend the spindles with a piece of tube. Back in the day that was how lots of trailer axles were made, you bought stubs and added tube to suit. As to the lack of suspension, also going back a few years now, around this area we had single axle trailers that held a bin full of approx 1500kg of citrus, solid axle, no suspension, no brakes and they used to tow them 2 at a time one behind the other fishtailing down the road. Dangerous as all hell but best I remember no one died
If its going on road best check the legalities in your state.
Cheers Andrew
-
23rd Feb 2018, 11:30 PM #4
I've done just what you are planning to do on my first ever trailer (still in use). It has been overloaded to bu99ery many times and the tubular axle is still straight.
On the other hand, I have seen many solid axles with sub axles welded on the OUTSIDE. It allows you to make good long deeply prepared multi-pass welds you can inspect, compared to a single weld on the outside edge of the tube,+ or - a few plug welds through holes in the tube..... As Leigh said, without suspension of some kind, you are only ever going to move it around your yard and on and off your trailer, not on the road.Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
24th Feb 2018, 12:31 AM #5Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Hi Simon, what you're proposing to do is quite normal, have googled a few pics for you. The drop varies according to the cutomers wishes, a semi drop, is where the stub is welded on top of the rest of the axle. You then have a ?" dropped axle which is where the axle is welded onto the axle with drop down plates of what size is required.
The beaut part about using this type of axle arrangement, is that the trailer can be set up level, and the drop worked out , particularly in your case, where the axle will be welded to the trailer.
It's perfectly legal, provided that it's done correctly, if arc welding, make sure that there are no slag inclusions, particularly if you're planning on taking it on the road, in which case I'd put some sort of suspension under it, otherwise it'll rattle everything loose.
If it's going to be for around the yard type of thing, DON'T lend it to anyone, unless you know it's going on a trailer. DAMHIKT.
Dropped Axle 2.jpg
Dropped trailer axle.jpg
Dropped trailer axle 1.jpg
Hope this helps,
KrynTo grow old is mandatory, growing up is optional.
-
24th Feb 2018, 06:15 AM #6Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Thanks everyone. The issue of no suspension does not worry me. It will mostly be used around my home however, I can't see why it cannot be towed as required. I have looked at many commercially made log splitters, some selling for over $10,000 and they don't have any suspension either.
https://www.tradefarmmachinery.com.a...-ws4150-495816
I was originally proposing to use some leaf spring suspension but it would have become a lot more complex. I then started looking at commercially available splitters and realised that none of them have suspension anyway.
WRT joining axles, I also found this on trailer sauce which is what prompted my question here but I wanted to hear what others have to say..
Trailer Sauce :: Building a Straight Beam Axle - Shim Method
Kryn, The method you suggested may be a good work around. I will have to have a look at the trailer heights etc. I had calculated for the axles to be welded under the cross member which would give me the calculated height of my worktable of about 950mm.
Cheers,
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
24th Feb 2018, 08:00 AM #7Diamond Member
- Join Date
- Mar 2014
- Location
- South of Adelaide
- Posts
- 1,225
Although i cant find it in VSB1 i'm pretty sure any trailer for use on the road must have suspension. I think the splitters you have seen are designed to be towed around a farm at low speed.
-
24th Feb 2018, 08:58 AM #8Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
Hi Snapatap,
I can't make comment either way about the regs because I have not actually looked. However, I find it hard to believe that someone would build a commercially made log splitter and sell it as legally towable and charge $17,500 if it were not actually legal...
https://www.ebay.com.au/itm/HYDRAULI...p2047675.l2557
Even the splitter I attached above states this:
Construction Specifications
Rugged heavy duty construction for a lifetime of trouble free use. Covered by 2 years warranty
Approved 50mm, 2000kg rated cast iron coupling
185 x 14 wheels & hubs. Handles all towing requirements
Neither of the above have suspension. I'm thinking I'm pretty safe?
Edit: I just looked at this document:
VicRoads' Registration requirements for light trailers manufactured ...
There is no reference to suspension requirements.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
24th Feb 2018, 10:03 AM #9Intermediate Member
- Join Date
- Feb 2018
- Location
- Loxton
- Age
- 54
- Posts
- 37
If you start to look around at all the things that are driven and towed on the road that don't have suspension you might be surprised how many there are. Around here tote bins for catching grapes from the grape harvesters are on the road all the time, no suspension on those, field bins, tractors, forklifts, earthmoving machinery........................ A bit like the proposed log splitter, non of these things are primarily meant to be on the road, but they get registered and driven on the road a little or a lot.
I would be pretty surprised if suspension was an absolute requirement for a trailer.
Cheers Andrew
-
24th Feb 2018, 10:35 AM #10
I followed a Chipper towed behind a 5 tonne truck on the highway. I was surprised to see it had no suspension! I don't know what weight it would have been but it was a tree surgeon's truck so I would assume that it was heavy. It seemed to travel fairly well but in corrugations at speed it may jump around a bit.
Just an aside....what grade of steel would trailer axle be? 4140? (Just for my own information)Just do it!
Kind regards Rod
-
24th Feb 2018, 10:46 AM #11Most Valued Member
- Join Date
- Aug 2011
- Location
- Melbourne
- Posts
- 4,779
HiChambezio,
I'm not sure the grade are of the particular ones I have but on my travels throught the net looking for information, I read that trailer axle steel range anywhere from mild steel (cheapie) to medium carbon steel such as 1045. It stated that anything harder than 1045 would potentially crack as it would not have the ability to flex with stresses encountered in normal use.
SimonGirl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.
-
24th Feb 2018, 12:49 PM #12Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Years ago, when I worked for a trailer place that made their own axles, the steel was called Duraflex this was about 45 years ago.
Copied this from the site below, if it helps.
This article explains the difference between DuraFlex and Mild Steel. More information can be found in the Article on Steel Grades.
What is Duraflex | call DIECUT on (03) 9544-9920
Duraflex (or Grade K1042 or K1045*)
*grade K1042 – made in Australia or New Zealand
*grade K1045 – made Overseas
Kryn
To grow old is mandatory, growing up is optional.
-
24th Feb 2018, 01:12 PM #13
-
25th Feb 2018, 01:54 AM #14
From Utility Trailer Axles, Spring Vs. Torsion: What's The Big Deal?
Torsion axles excel in applications like:
- Unusually bumpy or rough roads
- High vibration applications (like wood chippers)
regards from Canmore
ian
- Unusually bumpy or rough roads
-
25th Feb 2018, 02:02 AM #15
Similar Threads
-
Independent suspension and stub axles
By DaveTTC in forum TRAILERS & OTHER FABRICATED STUFFReplies: 28Last Post: 8th Nov 2016, 07:18 AM -
Cheap trailer axles
By jhovel in forum TRAILERS & OTHER FABRICATED STUFFReplies: 2Last Post: 24th Dec 2014, 12:42 AM -
extending frame of tandem trailer
By firstchoicecp in forum TRAILERS & OTHER FABRICATED STUFFReplies: 5Last Post: 16th Oct 2012, 05:00 PM -
Stub axles and using RHS for the axle
By surfin in forum TRAILERS & OTHER FABRICATED STUFFReplies: 9Last Post: 3rd Jul 2010, 12:58 PM -
6 stud toyota stub axles for trailer
By YarrD in forum TRAILERS & OTHER FABRICATED STUFFReplies: 35Last Post: 10th Aug 2009, 11:59 PM