Thanks: 0
Likes: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 4 of 4
Thread: Bending Galv Pipe
-
6th Jul 2016, 10:29 PM #1
Bending Galv Pipe
I need to fence in my back yard to keep a large dog in. I am using NB 40 galv steel posts for the corners etc and galv star droppers for the rest. The fence will be 1800mm high. I need to get some brace bars for the posts. I could get these bent to shape or I could buy a hydraulic pipe bender and do it myself. The shape I am thinking of is a 45 deg bend at the top and bottom, copied from the local tennis courts.
What do I need to bend NB 32 galv pipe? Will one of these be good enough?
NEW 12 TON Hydraulic Pipe Bender With 6 Dies Bending Jack Machine | eBay
Dean
-
6th Jul 2016, 10:53 PM #2
Will it do the job?.....in a word .....NO
The pipe that is offered for us to buy currently is too thin to bend using that type of bender. I have one the same and have had it for years but can't use it on new pipe. What I do is scrounge any old, even second hand pipe, usually ½" or ¾" or 1" and use it to make a bend then but weld it onto the new pipe. Tedious, yes, but you can get the desired effect
To bend the new pipe you would need a former front and back on the bender, some thing like an exhaust manufacturer would have. The pipe without the back former will just crushJust do it!
Kind regards Rod
-
6th Jul 2016, 11:23 PM #3
Thanks for that info. I remember a thread about this now. I will have a look and see what I have in the way of old pipe.
Dean
-
7th Jul 2016, 02:05 AM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,945
Dean, one of the biggest problems is the dies, they are imperial and new pipe is metric. It mightn't be much, maybe a mill, but the dies need to be a tight fit on the pipe, so that it is supported on the top and bottom, to get around this, I've used thin sheet metal just wide enough to cover a little over half the circumference of the pipe to reform the die, so that it fits a lot better. If the strip is too wide it won't allow it to stretch into shape. If the dies were too small it wouldn't be a problem to machine them out, but not so.
You should be able to buy metric dies, from where I don't know, the other alternative is to machine some out of solid plate.
KrynTo grow old is mandatory, growing up is optional.
Similar Threads
-
bending Gal. pipe - how to
By morrisman in forum METALWORK GENERALReplies: 32Last Post: 4th Jul 2016, 09:37 PM -
hydraulic pipe bending probs
By meadow street in forum METALWORK GENERALReplies: 2Last Post: 12th Dec 2013, 09:28 PM -
Bending 2 inch gal Pipe.
By Timless Timber in forum METALWORK GENERALReplies: 38Last Post: 20th Sep 2013, 09:31 PM -
Pipe Bending Fail
By BenM78 in forum METALWORK GENERALReplies: 33Last Post: 15th Aug 2011, 07:14 AM -
Bending brass pipe and flats
By STAR in forum METALWORK GENERALReplies: 7Last Post: 31st May 2008, 07:14 PM