  1. #1
    Join Date
    Sep 2007
    Location
    Adelaide
    Posts
    26

    Default MIG Wire (what brand do you use?)

    I have a little 120A WIA gasless welder and am due to replace the wire role. I have been looking at all the available brands out there and I can't decide what to buy.

    I am running .9mm wire & tips at the moment and have a good sized job comming up soon extending about 28 posts with wall thickness around 1.6mm.

    So here's a chance to let me and everybody else out there know what experiences you've had with different brand wires. I know I only have gasless but others might find it useful if any and all types of wires were discussed..

    Lastly sorry if this has been covered elsewhere, I had a bit of a look and couldn't really find what I was after.


    Cheers

  2. #2
    Join Date
    Oct 2006
    Location
    Armidale NSW
    Age
    52
    Posts
    915

    Default

    I run 0.6mm wire and the original spool of wire that came with my welder was really good and never had any troubles with it (it's a Kemppi welder, but I don't know what brand the wire was).

    When that spool ran out I got a BOC spool and I don't think it performs quite as well as the unknown one. The problem I have is with the ease at which it seems to want to kink - it doesn't happen all the time, but enough to be frustrating (and yes I've cleaned and/or replaced everything associated with the wire feed to try and fix the problem).

    Having said that though, that is the only downside I have found with the BOC wire and the 0.9mm wire should be less susceptible to kinking than the 0.6mm.
    Cheers.

    Vernon.
    __________________________________________________
    Bite off more than you can chew and then chew like crazy.

  3. #3
    Join Date
    Jan 2008
    Location
    Sydney
    Posts
    53

    Default

    I use and recommend Lincoln , but I use flux core rarely .

  4. #4
    Join Date
    Feb 2005
    Location
    Melbourne, Australia
    Age
    46
    Posts
    83

    Default

    CIG Weld
    I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones.
    Albert Einstein

  5. #5
    Join Date
    Aug 2005
    Location
    Victoria
    Posts
    9

    Default

    CIG Weld is too expensive. I got a roll 4 times as long from a place in Greens Rd Dandenong for the same price as the CIG Weld. It seems to be good wire.

    Tools

  6. #6
    Join Date
    Feb 2005
    Location
    Melbourne, Australia
    Age
    46
    Posts
    83

    Default

    Quote Originally Posted by Tools View Post
    CIG Weld is too expensive. I got a roll 4 times as long from a place in Greens Rd Dandenong for the same price as the CIG Weld. It seems to good wire.

    Tools
    Would this be it? How much for a 15kg roll?

    Migwell Australia
    88 Greens Road, Dandenong, VIC 3175
    p: (03) 9792 0055 f: (03) 9792 0800
    http://www.migwell.com.au
    Email Migwell Australia
    I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones.
    Albert Einstein

  7. #7
    Join Date
    Aug 2005
    Location
    Victoria
    Posts
    9

    Default

    Yes, that was the place. I didn't buy a 15kg, so don't know the price of them. Worth giving them a call though. I found it worth the trip from the inner city .

    tools

  8. #8
    Join Date
    May 2008
    Location
    Australia, Qld, Toowoomba
    Posts
    50

    Default What welding wire to buy and use?

    What welding wire to buy and use?

    Have a look at my website, click on the mig welding wire tab on the left hand side.

    I have written an article about that. What to look for when purchasing a quality mig wire.

    Peter


  9. #9
    Join Date
    Dec 2004
    Location
    Northen Rivers NSW
    Age
    57
    Posts
    131

    Default

    I have never had a problem with CIG gasless wire. Have had issues with cheaper brands.

    Get what you pay for i suspect.


  10. #10
    Join Date
    May 2008
    Location
    Australia, Qld, Toowoomba
    Posts
    50

    Default

    I have a saying. "Those who buy on price and price only. Get what they pay for."


    There is a lot of rubbish wire out there these days. Finding a good one is hard. One of the biggest problems is that many brands of wire are not actualy made buy the name that is on the box.

    ie. is BOC or WIA the manufacturer of that wire? or do they just get it from a manufacturer in china, italy hungary etc etc.


Similar Threads

  1. Respooling MIG wire
    By Andy Mac in forum WELDING
    Replies: 17
    Last Post: 9th Nov 2008, 06:42 PM
  2. Can you use Mig wire for Tig filler?
    By Rossluck in forum WELDING
    Replies: 6
    Last Post: 9th Jun 2006, 06:38 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •