    Default Is it possible to cut with an arc welder?

    Hi- having to cut some shapes out of a stack of corrugated iron.- far too much to do by hand snips and the curves are too sharp for grinding. Is it possible to use an arc to cut the iron, or better to hire an oxy.
    I've used an arc a bit many years ago, but haven't ever used an oxy?
    Steve:confused:

  2. #2
    Join Date
    Aug 2002
    Location
    Melbourne, Victoria
    Posts
    559

    Default

    Oxy would be much better than arc - especially on thin stuff, but you can get arc rods specific for cutting (exothermic cutting rods). They are very aggressive.

    What about a nibbler - fits to your drill and can cut very precise shapes, tight curves etc. Can be bought from bunnies,

    and sounds more suitable to your task. You can also get pneumatic ones.

    "Clear, Ease Springs"
    www.Stu's Shed.com


  3. #3
    Join Date
    Jun 2006
    Location
    Vic
    Posts
    5,629

    Default

    I would go with the nibbler.
    An arc or oxy would generate to much heat and buckle your sheets. Also depending on what the sheets are made from, the heat from the oxy or arc will make alot of dangerous fumes
    Cheers

    DJ


    ​ADMIN

  4. #4
    Join Date
    Oct 2006
    Location
    brisbane
    Posts
    1

    Wink 2 thoughs....

    Hi sprices ,if have the amps (160A maby) you could use a gouging electrode. Something like a 2.5mm UTP 85 would do it . As long as its ferrous theres no probs on what material is . It may cause a little distortion and be a little bit rought, but if you alowed for it you may be able to just grind it back .... or a cabon arc but that needs a compressor and the hand piece , the gougers are just electrods and you local welding supply place should have some , just a thought

  5. #5
    Join Date
    Oct 2006
    Location
    Victoria
    Posts
    1

    Smile thanks

    Thanks for the advice - have been thinking of a nibbler or power metal shears as better alternitives too.
    Steve

  6. #6
    Join Date
    Apr 2002
    Location
    Brisbane
    Posts
    429

    Default

    YEH you can cut sheet metal with an arc welder........ .... a mate of mine tried it at one stage. but its realy realy uggly and hot stuff goes everywhere.:eek: :eek:

    Tightly button you collar and pour a jug of water down you jocks first :eek: :eek: .
    Uise the bigest rod yor welder will take and crank the amps all the way up.

    you will be just blowing holes.

    realy nasty, not recomended and definitely a fire hasard.

    I'm having a good laugh just at the thaught of this bloke trying to shake sparks out of his jocks.

    but it does work.

    Seriously there has to be an easier way..... its called a plasma cutter.

    cheers
    Any thing with sharp teeth eats meat.
    Most powertools have sharp teeth.
    People are made of meat.
    Abrasives can be just as dangerous as a blade.....and 10 times more painfull.

  7. #7
    Join Date
    Jul 2003
    Location
    On the Downs, Darling SEQld
    Posts
    10

    Lightbulb

    Quote Originally Posted by soundman View Post
    I'm having a good laugh just at the thaught of this bloke trying to shake sparks out of his jocks.

    cheers
    I've seen the result of Slag down a Boot..................
    NOT GOOD!!!!

    Actually, heaps of water down the Boot was the best cure.
    By the time one has removed their boot,
    The damage is done; the Slag has lost its heat to ones FLESH:mad: :mad:
    3rd Degree burns, which most often Ulcerate and / or go Septic to some degree

    Arc weld [CUTTING] is BS as far as I'm concerned
    Navvi

  8. #8
    Join Date
    Sep 2006
    Location
    Avoca Victoria
    Age
    81
    Posts
    7,792

    Default

    Love this stuff!
    A nibbler or a plasma cutter is the definite safe recommendation, but if you really want it done in a hurry, with an aereonautical display of pyrotechnics, soak some 2.5mm rods in water overnight....rack up the amps...and go for it!
    Won't be accurate....you will need fire precautions...but it will cut.
    Please pretend it wasn't me that posted this....but I've cut 6mm plate in an emergency using this method.

    Regards,
    I wish I was anonamous! (where's the spell checker??)

  9. #9
    Join Date
    Oct 2006
    Location
    clothiers creek
    Posts
    5

    Default

    yep you can cut with a arc welder but on thin gauge stuff its best to use a nibbler or something because its messy and not very accurate . ive also cut thinck steel when i was in a paddock and run out of oxygen to cut with , so used the arc welder had it at over 200 amps blowing holes ina excavator bucket to weld a patch in . wasnt very neat but got the job done . i had little burn holes everywhere . :eek:

Similar Threads

  1. Current set up for your Mig
    By Grahame Collins in forum WELDING
    Replies: 23
    Last Post: 7th Jul 2006, 11:29 AM
  2. GMAW Welding For The DIYer
    By Grahame Collins in forum WELDING
    Replies: 8
    Last Post: 21st Dec 2005, 03:53 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •