Tips for welding in a narrow space (gap)
I volunteered to try to repair an aluminium step pulley (A series) that had part of the flange cracked off
P1040374.JPG
I did it by smoothing out the break, cutting a bit of sheet to suit, welding up and then machining the profile back. It sort of worked - the first go was a bit ropy (below) so tried again and was a little more successful
P1040379.JPG
I suspect that the alloy was a casting alloy so the higher silicon would not help, but I did have trouble getting a good bead in between the flanges. I tried switching to a gas lens, and that helped cover the longer than usual stick out that I had to use, but would be interested to know from members who have done this sort of thing before if there was a better/ more reliable/ easier way of doing this.
Plan B was to machine the whole flange off and weld a new one on, but I suspect that although the welding would be easier, the wedging action of the belt would cause problems down the track.
Thanks, Michael
-
16th Dec 2018, 01:21 PM #2Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
-
16th Dec 2018, 06:45 PM #3
I have heard of people heating the tungsten and putting a slight bend in it to aim the arc better but have never tried it myself.
-
16th Dec 2018, 11:49 PM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
If it were me, I'd fill it completely by TIG welding the break out. The excess can be machined out, and you'll have a smooth finish. Kryn
To grow old is mandatory, growing up is optional.
-
17th Dec 2018, 07:01 AM #5Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,559
I was a bit concerned about how much heat would be needed to do that. The large missing piece was 5mm thick and 20mm wide - a lot of molten metal in a small space. Would probably distort the flange.
Michael
Similar Threads
-
Welding Tips and Tricks
By Blu_Rock in forum WELDINGReplies: 6Last Post: 31st Jan 2016, 01:06 PM -
CIG Colt welding tips
By Gavin Newman in forum WELDINGReplies: 3Last Post: 10th Dec 2010, 01:19 PM -
CIG Colt welding tips
By Gavin Newman in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 6th Dec 2010, 10:04 PM -
Tips and tricks for welding
By matthew_g in forum METALWORK GENERALReplies: 1Last Post: 10th Jun 2010, 12:38 AM -
Hobart Welding Tips
By wheelinround in forum METALWORK GENERALReplies: 0Last Post: 20th Aug 2009, 02:11 PM