Which paint for welds on galv?
Hello All
I've been using Wattyl Cold Galvit aerosol on my welds on galvanised pipe farm gates, yards etc
Before spraying it on, I clean up the weld and HAZ with a wire wheel in a drill. Then I apply 3 coats 24 hours apart.
After a while ( 3 -5 years) the welds start rusting.
Can anyone point me to a superior product?
TIA
Graeme
-
29th Sep 2018, 06:55 PM #2Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,189
Welcome to the Forum Graeme.
3/5 years is not that bad considering they're outside fully exposed to the weather.
Bunbury, anywhere near the beach?
If the welds aren't smooth and allow water to sit in the welds that won't help.
For outside I usually use brush on cold galv as it produces a much thicker coating.
-
29th Sep 2018, 06:59 PM #3Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
What are you using for a top coat? I remember being told once that primers can have some porosity to them, so a top coat should be used to seal them.
Michael
-
29th Sep 2018, 08:22 PM #4Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
If my memory serves me correct, cold galv paint has to be about 1mm thick to afford the same protection as hot dipped Galvanising. It was brushed on.This was about 50 years ago on a grain silo construction site at Pt Giles on the Yorke Peninsula.
KrynTo grow old is mandatory, growing up is optional.
-
29th Sep 2018, 10:23 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
-
29th Sep 2018, 10:44 PM #6
You need to use brush on cold gal followed by an aerosol spray to seal. I’ve had good results following this regime at my uncle’s farm, not as shiny after several years but no rust showing. The only spots showing rust is where the livestock has worn the paint and also the original gal coating away
Cheers
DJ
-
29th Sep 2018, 11:23 PM #7Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Similar Threads
-
Bending Galv Pipe
By Oldneweng in forum TRAILERS & OTHER FABRICATED STUFFReplies: 3Last Post: 7th Jul 2016, 02:05 AM -
Galv steel centreboard
By hereselmo1 in forum METALWORK GENERALReplies: 20Last Post: 10th Jun 2011, 11:26 PM -
Pulleys... Paint or no paint?
By Com_VC in forum THE HERCUS AREAReplies: 5Last Post: 3rd Apr 2011, 08:42 PM -
How many welds?
By Single-phase in forum WELDINGReplies: 7Last Post: 24th Oct 2009, 04:23 PM -
Hot dip galv question from the newbie
By aaron 01 in forum METALWORK GENERALReplies: 3Last Post: 26th Feb 2009, 12:49 AM