    Default hardened shaft repair

    Hi all, i have an Ozito brand multi head cordless tool, and the chainsaw head component suffered a snapped drive shaft due to a slight kickback. the internal components look like reasonable quality, though badly designed in not having some shear point in the design. anyhow….i am going to try a tig repair and just after some reassurance that it is possible. what filler rod would be best. i have 316L stainless and comweld high test or woul something else be better. i have ground the ends to a V in preparation and just awaiting some encouragement. it is only a home use machine but would be a shame to junk it. shaft is approximately 8mm dia.CBB8870E-E8FF-4C4A-A8E1-84B2B04CAC23.jpg483BF918-F11B-44A4-9A47-07D4FCEEE08C.jpg

  2. #2
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,658

    Default

    I am not a welder although have completed very similar projects in the past I would go with hitest if you weld with any thing other than TIG you most likely need to re case harden ( in my experience being Ozito it will only be case hardened )

    I assume it is past it's 5 year warranty

  3. #3
    Join Date
    May 2008
    Location
    Perth
    Posts
    241

    Default

    Alternative option, since it's Ozito, there's a good chance you could get Bunnings to special order in that part. I've done so in the past, when the cutting head in my frond chomper got chewed up.

  4. #4
    Join Date
    May 2022
    Location
    Grafton NSW
    Age
    68
    Posts
    5

    Default

    Quote Originally Posted by LordBug View Post
    Alternative option, since it's Ozito, there's a good chance you could get Bunnings to special order in that part. I've done so in the past, when the cutting head in my frond chomper got chewed up.
    thanks, i will give it a try.

  5. #5
    Join Date
    May 2022
    Location
    Grafton NSW
    Age
    68
    Posts
    5

    Default

    Quote Originally Posted by China View Post
    I am not a welder although have completed very similar projects in the past I would go with hitest if you weld with any thing other than TIG you most likely need to re case harden ( in my experience being Ozito it will only be case hardened )

    I assume it is past it's 5 year warranty
    thanks china, yes the warranty has gone. it looks like it broke along a fault line of sorts. i should be able to get a decent weld on it though.
    Attached Images Attached Images

Similar Threads

  1. Hardened Bastard
    By Doctor Bungle in forum METALWORK GENERAL
    Replies: 8
    Last Post: 6th May 2021, 10:43 PM
  2. Hardened Drill Guides
    By KBs PensNmore in forum WANTED TO BUY
    Replies: 8
    Last Post: 7th Sep 2020, 09:07 PM
  3. Masport chipper/shredder shaft repair
    By OxxAndBert in forum METALWORK PROJECTS
    Replies: 24
    Last Post: 11th Oct 2019, 05:19 AM
  4. Machining case hardened shaft
    By Bryan in forum METALWORK GENERAL
    Replies: 27
    Last Post: 3rd Nov 2010, 04:42 PM
  5. Shaft repair
    By Bryan in forum METALWORK GENERAL
    Replies: 9
    Last Post: 9th Jun 2010, 08:44 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •