hardened shaft repair
Hi all, i have an Ozito brand multi head cordless tool, and the chainsaw head component suffered a snapped drive shaft due to a slight kickback. the internal components look like reasonable quality, though badly designed in not having some shear point in the design. anyhow….i am going to try a tig repair and just after some reassurance that it is possible. what filler rod would be best. i have 316L stainless and comweld high test or woul something else be better. i have ground the ends to a V in preparation and just awaiting some encouragement. it is only a home use machine but would be a shame to junk it. shaft is approximately 8mm dia.CBB8870E-E8FF-4C4A-A8E1-84B2B04CAC23.jpg483BF918-F11B-44A4-9A47-07D4FCEEE08C.jpg
-
29th May 2022, 04:08 PM #2China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
I am not a welder although have completed very similar projects in the past I would go with hitest if you weld with any thing other than TIG you most likely need to re case harden ( in my experience being Ozito it will only be case hardened )
I assume it is past it's 5 year warranty
-
29th May 2022, 08:10 PM #3Tool addict
- Join Date
- May 2008
- Location
- Perth
- Posts
- 241
Alternative option, since it's Ozito, there's a good chance you could get Bunnings to special order in that part. I've done so in the past, when the cutting head in my frond chomper got chewed up.
-
29th May 2022, 08:49 PM #4New Member
- Join Date
- May 2022
- Location
- Grafton NSW
- Age
- 68
- Posts
- 5
-
29th May 2022, 09:07 PM #5New Member
- Join Date
- May 2022
- Location
- Grafton NSW
- Age
- 68
- Posts
- 5
Similar Threads
-
Hardened Bastard
By Doctor Bungle in forum METALWORK GENERALReplies: 8Last Post: 6th May 2021, 10:43 PM -
Hardened Drill Guides
By KBs PensNmore in forum WANTED TO BUYReplies: 8Last Post: 7th Sep 2020, 09:07 PM -
Masport chipper/shredder shaft repair
By OxxAndBert in forum METALWORK PROJECTSReplies: 24Last Post: 11th Oct 2019, 05:19 AM -
Machining case hardened shaft
By Bryan in forum METALWORK GENERALReplies: 27Last Post: 3rd Nov 2010, 04:42 PM -
Shaft repair
By Bryan in forum METALWORK GENERALReplies: 9Last Post: 9th Jun 2010, 08:44 PM