Thanks: 0
Needs Pictures: 0
Picture(s) thanks: 0
Results 1 to 4 of 4
Thread: Tig water cooling
-
13th Feb 2018, 09:40 AM #1Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,255
Tig water cooling
I suspect that all these are is a fan forced coil with a small pump to circulate water.
Would this be correct?
If so I have some small coils from scraped aircon units that may suit if some one would like to explore the possibility of making one for themselves
20170908_163215[1].jpg
message me if interested
-
13th Feb 2018, 10:02 AM #2Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
This Old Tony did a good video about modifying a unit he was given, which is a good guide as to how they're put together.
https://www.youtube.com/watch?v=x2ai5eDzvxU
The one feature I wouldn't have thought of is the flow alarm, which makes sense, since if the flow stops and you don't realise, the torch could heat up and melt pretty quickly.
-
13th Feb 2018, 12:59 PM #3Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,183
Thanks for the link to the vid, Old Tony has a funny way of putting things which adds to the viewing experience.
-
16th Feb 2018, 08:15 AM #4Senior Member
- Join Date
- Jan 2015
- Location
- Sydney
- Posts
- 211
I made a tig cooler for my tig, holds about 10l, radiator and a thermo fan on a controler to turn on if it gets too hot.
If i was to do it again, i would make it half the size maybe even less, probably 3l to make it more portable and get a smaller radiator.
Ive never had the temp rise more then 5 degrees above ambient, even on ac.
Im even tossing up the idea of making another cooler as the pump im using is quite noisy and vibrates. (12v diaphram pump)
Sent from my SM-G935F using Tapatalk
Similar Threads
-
ASEA motor with broken cooling fan
By paul33 in forum ELECTRICALSReplies: 5Last Post: 26th May 2017, 06:41 PM -
Mist Cooling / Cutting Lubrication Question ..... ?
By RoyG in forum METALWORK GENERALReplies: 32Last Post: 9th Jul 2016, 08:28 PM -
Cooling down a mini-mill motor
By Jors in forum METALWORK GENERALReplies: 5Last Post: 15th Jan 2013, 09:10 AM -
flood cooling
By tanii51 in forum METALWORK GENERALReplies: 7Last Post: 5th Mar 2010, 09:18 PM -
Cooling while cutting
By BobL in forum METALWORK GENERALReplies: 8Last Post: 7th Mar 2007, 12:42 AM