Can I weld stainless sheet with a stick or gas welder
I'm making a device called a Smokenator for my Weber kettle, they are are available online but at around $300 they are a bit out of my price range just to see if they are any good. The pics shown are of the factory unit, mine looks decidedly home made but should work just as well assuming they do indeed work as promised.
I've bent up a piece of stainless and cut it to fit inside the kettle and now need to weld two tabs on to hold it in position, I don't have a tig just a gas and stick welder not wanting to make a hash of it and make it look even more home made my question is will either of my two welders do stainless, if not then I don't even want to try, the stainless is 1.2mm thick.Smokenator 2.JPGSmokenator.JPG
-
11th Dec 2017, 08:24 PM #2Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,563
You can get stainless rods for a stick welder but they are expensive and would be difficult to use on 1.2mm I suspect.
Stainless steel rivets are readily available though. Is the design flexible enough to allow you to use a couple of those?
Michael
-
11th Dec 2017, 09:42 PM #3
Whereabouts in Adelaide are you? Would it be easier if one of us with TIG welded it up for you?
-
11th Dec 2017, 11:00 PM #4Most Valued Member
- Join Date
- Nov 2017
- Location
- Geelong, Australia
- Age
- 57
- Posts
- 2,673
I've successfully used 1.6mm stainless rods on 1.6mm stainless exhaust tube, and I reckon if you're reasonable with your stick welder you'd be OK to use them for small welds on 1.2 - assuming your design can take a lapped joint. I definitely wouldn't be keen to butt weld with them.
You can get small packs of stainless rods with a few assorted size rods in them, maybe 8 or so total. Pretty sure even Bunnings has them. I can't recall the price but from memory it worked out a couple of dollars per rod so expensive in per-rod terms, but for the occasional small stainless bracket etc quite cheap.
I'm sure the pro's have a better suggestion or skills, but here's what I'd do in your situation:
Make the bracket up with a tab that laps over the other part, and drill a couple of holes about a 3mm (guessing size...) in the tab that's underneath/behind - ie out of sight.
Grab a lump of copper or aluminium to use as a backing bar to resist blowing a hole straight through, and then give it a very quick tack in the hole, basically creating a miniature puddle weld.
Hopefully you've got a couple of bits of scrap to practice the technique on before letting loose on the real job.
If that's too scary, I'd second Michael's suggestion to rivet them on.
Even better if someone local volunteers to TIG them for you.
Steve
-
12th Dec 2017, 12:52 AM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
If by "gas welder" you mean oxy/acetylene yes you can
-
12th Dec 2017, 09:46 AM #6Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
Yes I have oxy acetylene. Is stainless fusion welding the same as mild steel fusion welding, possibly I could cut some thin strips of the stainless from the offcuts and use this as filler, will I need a flux ?
Rivets are an option - I can turn some up from a few of the stainless screws left over from the deck.
Before I had the Oxy set I had successfully arc welded exhausts in the past by "pecking" or stitching the weld (only way I can describe it) - and if stainless rods are available in small quantities (5 or 6) could give this a go - is stainless arc welding the same as mild steel welding ?
-
12th Dec 2017, 09:52 AM #7
If you need some SS filler rods to play with the oxy/acetylene I can supply some for nothing as I have plenty here. I'm at Aberfoyle Park if that helps.
Alternatively, bring the bits up here and I'll glue them together with the TIG.
-
12th Dec 2017, 11:08 PM #8Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
That is a kind offer Gavin I'll send you a private message.
-
13th Dec 2017, 09:29 AM #9
No problems, reply sent.
-
13th Dec 2017, 09:39 AM #10Banned
- Join Date
- Feb 2015
- Location
- Oz
- Age
- 73
- Posts
- 459
You can also weld stainless with ordinary rods. If rust isn't a problem, this is the cheapest way around it.
-
15th Dec 2017, 09:04 AM #11Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
It will go inside a BBQ kettle so decided to use stainless like the commercial version, I did cut a small 1mm wide length from one of the offcuts and tried it as a filler - went just like normal mild steel fusion welding, seems I was concerned about nothing, the only drawback here is that I can only get short bits around 50mm long to use as filler and need to hold with pliers.
Thanks to Gavin's kind offer I now have a couple lengths of stainless rod, I'll post a pic once done.
-
15th Dec 2017, 12:01 PM #12
A concern I would have would be warpage of your stainless steel sheet . I would be inclined to use lots and and lots of tacks.
Use as few KPAs on the gauge( 30 Kpa on both Oxy and Acet) as you can get away with and weld with a nuetral flame and flux if you can get it
Also go down a size in the nozzle diameter to what you would use for steel.
Avoid a full weld as in a complete pass. Do 25mm then go to somewhere else and do a bit there.You don't want to concentrate the heat in one spot.
I saw a sheety cut slivers with a sheet guillotine to use as filler when he he could not get a hold of filler wire.
Best of luck as this can be a difficult process on this material.
Grahame
-
15th Dec 2017, 12:10 PM #13
If you have oxy, then silver soldering would be my choice of process. Stainless silver solder beautifully and a Weber won't be hot enough to melt it.
Cheers, Joe
retired - less energy, more time to contemplate projects and more shed time....
-
15th Dec 2017, 12:27 PM #14Golden Member
- Join Date
- Dec 2007
- Location
- Adelaide
- Posts
- 575
Thanks for all of the replies and encouragement.
Pic of welds attached - I bent the sheet with my folder so the welds required are only short where the tabs are attached - around 20mm long, so no issues with warp, the commercial version is all in one piece which would have been nice if I could have done it. I'm a bit hampered as I now need glasses but they won't fit with my goggles so had to weld with either no glasses or no goggles - I chose no glasses - it's a PIA when your eyesight starts to go south, weld looks ok me I tried to break it off but just bent the tab. Used a carburising flame, the only flux I have is for bronze welding and also silver soldering so did not use any.20171215_110650.jpg20171215_110704.jpg
-
16th Dec 2017, 03:20 PM #15Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Similar Threads
-
Attempting to Join a Thin Sheet of Stainless to a Slightly Thicker Sheet?
By mattegan in forum METALWORK GENERALReplies: 7Last Post: 25th Jun 2016, 03:46 PM -
Mig welding Stainless Steel tube and Sheet
By garfield in forum WELDINGReplies: 20Last Post: 26th May 2016, 09:26 AM -
Can someone post a video of how they can weld thin square tube with a stick welder?
By Njmpm in forum WELDINGReplies: 34Last Post: 17th May 2015, 10:39 PM -
QUEENSLAND Cig welder transarc tradesman HD (stick/arc welder) 3phase
By dkaoffroad in forum METALWORK - Machinery, Equipment, MARKETReplies: 0Last Post: 8th Jun 2013, 10:45 AM -
#mill sheet weld ..help required from MIG masters!
By NewLou in forum WELDINGReplies: 3Last Post: 5th Jan 2008, 04:38 PM