Results 16 to 20 of 20
Thread: Welding Table top
-
22nd Nov 2017, 05:10 PM #16Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
Okay...here it is before i put the top on it20171122_151444.jpg
-
23rd Nov 2017, 03:26 PM #17Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Slight hijack-
I'm also looking at building a welding table. Where can I get 12mm steel plate cut to size on the south side of Melbourne? I'd like a nice finish on the edges, which I assume means cutting with a water jet?Chris
-
17th Mar 2018, 11:48 AM #18Most Valued Member
- Join Date
- Jul 2006
- Location
- Athelstone, SA 5076
- Posts
- 4,258
This is where I am at the moment. Am going to make a draw for the bottom and then paint.....but dont hold your breath...lol
20180316_144521[1].jpg
20180316_144511[1].jpg
20180316_155909[1].jpg
The extra steel plate on the top is for another project.....when I get tuit
-
17th Mar 2018, 01:09 PM #19Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,959
Thanks for the pics, looks great, the way everything is on the one bench and can be moved around.
My only concern would be the acetylene cylinder sitting under the bench, if it's not turned off properly, there could be a problem with sparks there!!!
KrynTo grow old is mandatory, growing up is optional.
-
17th Mar 2018, 03:59 PM #20Member: Blue and white apron brigade
- Join Date
- Feb 2006
- Location
- Perth
- Posts
- 7,188
It depends what you are welding and if you weld directly to your top.
I had a similar dilemma about 6 years ago when I made my lightweight 600 x 900 mm topped welding table.
On top of the frame I temporarily placed two pieces of 700 x 450 mm x 6mm steel pieces and they have been there more or less ever since.
I leave a 50 mm slot between the sheets for increased clamping edges
When larger piece of metal have to be clamped down I take the pieces off and clamp to the bench frame because it's now possible to clamp to more spots than the outer edge of the sheets
When welding small pieces I tend to use a (removable) offset 6" vice to hold the work, or clamp to the edges of one of the sheets.
The easily removable vice on that table has been a real winner.
BTW that bench has a lot more bracing on it now including a 5th leg directly under the vice.
After doing this for 6 years the only thing I would change is perhaps use thicker pieces of plate?
Things would be different if I was welding lots of HD and/or larger objects and I would then start with a much bigger HD table.
Similar Threads
-
FixturePoint Welding Table 900 x 600mm Table
By dradyz in forum METALWORK - Machinery, Equipment, MARKETReplies: 2Last Post: 26th May 2016, 01:38 PM -
Topping a welding table
By th62 in forum METALWORK GENERALReplies: 11Last Post: 18th Aug 2014, 11:22 AM -
Steel plate for welding table
By th62 in forum WELDINGReplies: 6Last Post: 18th Aug 2014, 09:18 AM -
Folding Welding Table
By bimbo in forum WELDINGReplies: 16Last Post: 2nd Jun 2012, 05:31 AM -
Welding table design
By quercus in forum WELDINGReplies: 37Last Post: 21st Mar 2009, 07:21 PM