    Okay...here it is before i put the top on it20171122_151444.jpg

  2. #17
    Join Date
    Nov 2007
    Location
    melbourne australia
    Posts
    3,228

    Default

    Slight hijack-
    I'm also looking at building a welding table. Where can I get 12mm steel plate cut to size on the south side of Melbourne? I'd like a nice finish on the edges, which I assume means cutting with a water jet?
    Chris

  3. #18
    Join Date
    Jul 2006
    Location
    Athelstone, SA 5076
    Posts
    4,258

    Default

    This is where I am at the moment. Am going to make a draw for the bottom and then paint.....but dont hold your breath...lol
    20180316_144521[1].jpg
    20180316_144511[1].jpg
    20180316_155909[1].jpg

    The extra steel plate on the top is for another project.....when I get tuit

  4. #19
    Join Date
    May 2011
    Location
    Murray Bridge S Aust.
    Age
    71
    Posts
    5,959

    Default

    Thanks for the pics, looks great, the way everything is on the one bench and can be moved around.
    My only concern would be the acetylene cylinder sitting under the bench, if it's not turned off properly, there could be a problem with sparks there!!!
    Kryn
    To grow old is mandatory, growing up is optional.

  5. #20
    BobL is online now Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    It depends what you are welding and if you weld directly to your top.

    I had a similar dilemma about 6 years ago when I made my lightweight 600 x 900 mm topped welding table.

    On top of the frame I temporarily placed two pieces of 700 x 450 mm x 6mm steel pieces and they have been there more or less ever since.
    I leave a 50 mm slot between the sheets for increased clamping edges

    When larger piece of metal have to be clamped down I take the pieces off and clamp to the bench frame because it's now possible to clamp to more spots than the outer edge of the sheets

    When welding small pieces I tend to use a (removable) offset 6" vice to hold the work, or clamp to the edges of one of the sheets.

    The easily removable vice on that table has been a real winner.


    BTW that bench has a lot more bracing on it now including a 5th leg directly under the vice.

    After doing this for 6 years the only thing I would change is perhaps use thicker pieces of plate?

    Things would be different if I was welding lots of HD and/or larger objects and I would then start with a much bigger HD table.

Page 2 of 2 FirstFirst 12

Similar Threads

  1. FixturePoint Welding Table 900 x 600mm Table
    By dradyz in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 2
    Last Post: 26th May 2016, 01:38 PM
  2. Topping a welding table
    By th62 in forum METALWORK GENERAL
    Replies: 11
    Last Post: 18th Aug 2014, 11:22 AM
  3. Steel plate for welding table
    By th62 in forum WELDING
    Replies: 6
    Last Post: 18th Aug 2014, 09:18 AM
  4. Folding Welding Table
    By bimbo in forum WELDING
    Replies: 16
    Last Post: 2nd Jun 2012, 05:31 AM
  5. Welding table design
    By quercus in forum WELDING
    Replies: 37
    Last Post: 21st Mar 2009, 07:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •