    Default MMA holding the electrode for better control?

    I have seen some Youtube videos whereby the Welder, wearing glove is holding the electrode. Is this a dangerous practice?

  2. #2
    Join Date
    Jun 2007
    Location
    sydney ( st marys )
    Age
    64
    Posts
    4,890

    Default

    Only if it burns your hand,

  3. #3
    Join Date
    Oct 2008
    Location
    Mole Creek
    Posts
    45

    Default

    Quote Originally Posted by topari View Post
    I have seen some Youtube videos whereby the Welder, wearing glove is holding the electrode. Is this a dangerous practice?
    Only if you grab the hot bit! MMA holding the electrode for better control?

    On a more serious note though, it's a quite safe and even recommend practice. Provided everything is dry (especially your gloves) there shouldn't be any problem.

    Typically, because of the low voltages involved and the relatively high resistance of the human body, the worst shock you'll get from a stick welding machine is an unpleasant tingle.

    I don't recommend this at all, but I have received a shock from the HF start of a TIG machine several times (as has just about everyone who's used one for more than a few hours) and it can leave a small burn, and it stings a bit fora little while, but no lasting damage.

    Cheers,... Jon.

    Sent from my Moto G (4) using Tapatalk

  4. #4
    Join Date
    Oct 2008
    Location
    Mole Creek
    Posts
    45

    Default

    Quote Originally Posted by pipeclay View Post
    Only if it burns your hand,
    Haha, beat me to it! MMA holding the electrode for better control?

    Sent from my Moto G (4) using Tapatalk

  5. #5
    Join Date
    Feb 2015
    Location
    Oz
    Age
    73
    Posts
    459

    Default

    Many, many, many years ago when I was working as a welder the shop used 1" x 1/8" steel strapping running from the welders earth terminal to the bench. If you happened to be leaning against the bench or standing on the earth when changing elelectrodes you'd get a boot. Back in the 60s health and safety issues weren't even thought of, shorts, T shirts, leather soled shoes and even thongs were the
    clothing for the day. I remember many a welder hopping around the shop because a bit of slag had found it's way into their boot. Every bench also had a 1 gallon tin next to the welder for electrode stubs, after a while you got to be a pretty good shot and you could twist and flip and hit the bucket from yards away, quite often some would fire at each other. Everyone had flash burns on the upper chest, neck and arms. Flash burns to the eyes and steel splinters in the eyes were also the order of the day. Those were the days - not!

  6. #6
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    For learners (and even for me in certain situations as I have something called essential tremor which causes my hands to shake) I cut rods half to improve control.

  7. #7
    Join Date
    Feb 2015
    Location
    Oz
    Age
    73
    Posts
    459

    Default

    Me too, much easier to control for me, trouble is you're forever changing rods.

  8. #8
    BobL is offline Member: Blue and white apron brigade
    Join Date
    Feb 2006
    Location
    Perth
    Posts
    7,189

    Default

    Quote Originally Posted by sacc51 View Post
    Me too, much easier to control for me, trouble is you're forever changing rods.
    Most of the stick and TIG work I do is small so short runs and so I'm stopping to re-setup/clamp work etc, so not that big a deal.
    I will still use a full length rod if it's a long run that is needed

  9. #9
    Join Date
    Jul 2013
    Location
    nsw
    Posts
    256

    Default

    just like playing pool or snooker it helps to have a good front prop.

    questicking

  10. #10
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    When welding in the horizontal or vertical position I sometimes support a fresh long electrode with a gloved finger.

    If you cut up a buggered glove, you can cut the fingers off and slide the (back of the hand) portion over the fingers of the supporting glove it makes a handy heat shield to rest the hot electrode on.

    The air gap between the two layers of leather allows for a reasonable temperature of your fingers inside your welding glove.

    Surprisingly, the slip on lasts longer than you think it would.

    Grahame

  11. #11
    Join Date
    Feb 2012
    Location
    Sydney
    Posts
    67

    Default

    As Grahame described, I also support a new long electrode with gloved fingers and gradually move the left hand up the rod until it's shorter, then remove the left hand altogether. For heat shielding I like the silver foil backed pad that slips over the back of the glove. Gunslingers may like smoking gloves but I'm not that keen on singed fingers.

  12. #12
    Join Date
    Jan 2004
    Location
    Mackay North Qld
    Posts
    6,446

    Default

    I tried the the gloves with woven aluminium foil but it did stink somewhat when it got hot.

    The leather on the cover glove got hot , dry and crusty but didn't pong to the extent that the Ali ones did. If there was an air gap between the inner and the outer,the heat was bearable.

  13. #13
    Join Date
    Aug 2011
    Location
    Melbourne
    Posts
    4,779

    Default

    When I first started welding I used to cut the electrode in half (as others have done) in order to improve control. I don't do that anymore but I recently (last week) watched a video where the guy held the rod with his other hand to improve control. I had never seen or done that before but have since tried that method and it helps. I just held it with welding gloves and let go when the rod gets shorter.

    I also find that WRT welding, I have good days and bad days. Some days I will pull off the sexiest weld bead ever seen (IMHO) and other days I can't weld for ! I also recently found that (unlike billards or pool) my welding ability is greatly reduced after a couple of ciders.

    Simon
    Girl, I don't wanna know about your mild-mannered alter ego or anything like that." I mean, you tell me you're, uh, super-mega-ultra-lightning babe? That's all right with me. I'm good. I'm good.

Similar Threads

  1. Electrode and amp settings?
    By benupton in forum WELDING
    Replies: 8
    Last Post: 25th Jul 2012, 06:58 PM
  2. aluminium arc electrode
    By barney702 in forum WELDING
    Replies: 9
    Last Post: 9th Jun 2011, 08:02 PM
  3. Arc inverter electrode + or - ?
    By Mathuranatha in forum WELDING
    Replies: 5
    Last Post: 28th Jun 2010, 09:32 PM
  4. Electrode positive or Electrode negative
    By .RC. in forum WELDING
    Replies: 8
    Last Post: 26th Apr 2009, 12:39 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •