Should be pretty straight forward pre flow and post gas maybe 3 - 5 seconds. Base current should be the main amperage control as any other welder would have. Peak current would be for pulse so you could set to minimum, down slope set to 0 Pulse width and Pulse Freq same thing. There should be a switch to turn pulse on or off so it won't really matter what they are set on if it is off. Clear Width? I think that was to do with cleaning, used with AC only. You could set this to minimum if you are only welding steel.
Hope this helps
-
4th Dec 2017, 01:08 PM #62Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Thanks mate that sounds easy cheers
I may have a bit of coin to play with soon so i was looking at buying a proper welder something of decent quality but not overly complicated, I'm looking for a light weight mig that can do aluminium, it must be a small unit so i can leave it inside the house
what are some options? so far i like the token tools synergic mig but its a little over the $1000 budget
so far to date my mig experience has been horrible sadly i have only bought cheap machines, my welds are horrifying so i would like to get a decent machine and sell my ESAB / Spool gun and go with something much smaller
i would also like to step away from the gasless wire and go with solid wire, the reason i want to go with a quality machine is i am still building that car trailer and to put it simple my welds put me off finishing the job i think its my welders that are the limiting factor
i have heard good reviews about the Mag Mate and also the UNIMIG Razor what are your thoughts guys?
-
7th Dec 2017, 06:53 PM #63Most Valued Member
- Join Date
- Aug 2009
- Location
- Sydney, NSW, Australia
- Posts
- 1,844
Those settings worked perfect i ran a bead first go on some 32x3mm round tubing than i had a few goes at the corner joint, once i left the gas off and it was hard to get it tacked and awkward positions i found it really hard to follow around the tube
machine is a bit iffy what the dial is reading now reads 109amps on the readout i had to keep bumping up the amps because i was under powered (i was going by the dial)
Similar Threads
-
Picked up another stray.
By DSEL74 in forum METALWORK GENERALReplies: 18Last Post: 3rd Jan 2017, 05:25 PM -
Picked up a McMillan MA15 Air compressor
By dorikin in forum METALWORK GENERALReplies: 16Last Post: 18th Sep 2014, 05:24 PM -
Manual for EMF/CIG Cigweld Transtig 250 Tig Welder AC/DC HF
By argeng in forum WELDINGReplies: 1Last Post: 20th Jul 2013, 09:25 AM -
Transtig 180 ac/dc welder
By kr_cf in forum WELDINGReplies: 47Last Post: 25th Oct 2012, 09:40 PM