New gear to TIG weld
What TIG gear should I buy for my BOC smootharc 130 (DC stick / lift TIG) welder to learn TIG welding?
So far I have read I need:
1) A torch ($50 from total tools?). Size 17 looks good, its what "This old Tony" uses.
2) Some gas (D size argon or a smaller bottle?) Buy or rent? I have no real conception of how much you use.
Anything else? Any recommended suppliers? Thanks.
-
16th Aug 2017, 06:14 PM #2Member
- Join Date
- Mar 2017
- Location
- wollondilly nsw
- Posts
- 62
Didnt you get a torch with the tig?
Buy the cylinder. You just exchange it for a full one and cost of gas. Can upscale it and pay difference at a later date too. Gasweld and a few others sell them
Sent from my SM-T355Y using Tapatalk
-
16th Aug 2017, 10:17 PM #3Senior Member
- Join Date
- Jan 2015
- Location
- Sydney
- Posts
- 211
For 130amps i would probably look at a wp9 torch. Much smaller and rated to 125amps. I run a wp20 which is the same but watercooled. As for gas maybe start of with the bunnings deal. If you are using heaps maybe look into buying your own e size.
Sent from my SM-G900I using Tapatalk
-
17th Aug 2017, 12:01 AM #4Tool addict
- Join Date
- May 2008
- Location
- Perth
- Posts
- 241
+1 to brendanh's recommendation of Bunnings for the argon. No rental cost, just a "deposit" on the cylinder and the refill cost ($80 or so? maybe a little more), so at worst if you crack the s***s at it you can get a large part of the outlay back, not sure if you can do that with any other cylinder seller. They only offer one size, but it's a fine size to get started on.
After that, you'll just need a regulator, and maybe a flowmeter if you want that bit of extra visual information.
-
17th Aug 2017, 07:45 AM #5Member
- Join Date
- Mar 2017
- Location
- wollondilly nsw
- Posts
- 62
Bunnings is $200 deposit and $99 for the refills for a D size. Shop around and do some economics. There are better options if you want to get serious with it. Also look on gummy etc as guys may be selling cylinders they have bought and no longer use.
Sent from my SM-T355Y using Tapatalk
-
17th Aug 2017, 08:41 AM #6Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,562
Check the manual - an industrial TIG machine will take a generic torch and so on, but some of these small machines that are technically capable of TIG* may require particular accessories to function. There may be a particular type of torch that you need to buy.
Michael
*Not denigrating them as not being capable, just that sometimes with machines/ devices that are 'multi-functional' (and not just welders) I get the feeling the marketing guys have pushed for more function/ features without wanting to spend the money to develop the enabling 'infrastructure'.
As an example, lift start means companies don't have to develop a HF start module (so cheaper) but experienced welders I've talked to have told me that it is easier to contaminate electrodes with that starting method if not done properly.
Another one is the MIG that is pushed as being capable of welding Al, even though the seller does not include the new rollers, liner,...
-
17th Aug 2017, 12:02 PM #7Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
Provided the unit has a stick/TIG switch it should be good to go - both modes are DC constant current, the switch just changes the current regulation profile.
Having dipped the tungsten plenty of times now, I've come to realise it isn't always a show-stopper, particularly with steel, so I can see why a lift or scratch start wouldn't necessarily be such a problem.
-
17th Aug 2017, 01:01 PM #8Senior Member
- Join Date
- Jan 2015
- Location
- Sydney
- Posts
- 211
Hf start isnt nessesery but it is nice to have.
Sent from my SM-G900I using Tapatalk
Similar Threads
-
Weld Art?
By newbyangler in forum WELDINGReplies: 20Last Post: 5th Jun 2016, 09:01 AM -
Weld Quality
By rod1949 in forum WELDINGReplies: 10Last Post: 15th Apr 2014, 05:01 PM -
Can you over weld ali?
By constablechris in forum WELDINGReplies: 18Last Post: 5th Feb 2012, 06:34 PM -
Gear tooth count on Back/Bull Gear.
By pipeclay in forum THE HERCUS AREAReplies: 31Last Post: 6th Jan 2010, 11:56 AM -
Metal gear / worm gear needed
By colinshannon in forum METALWORK GENERALReplies: 14Last Post: 29th Mar 2007, 10:49 PM