Need help - welding on trailer hinges - Canberra
I've just about finished my box trailer renovation, all done but I've got to weld the new barrel hinges I have here onto the two trailer gates. The old hinges rusted to seizure down the coast, I had to grind them off.
I'm ready to go, so I went on to Gumtree where a fellow nearby in northside Canberra had been advertising small backyard jobs, he'd said $30 to do the job. Great, but that was last October and now I'm back on Gumtree he's nowhere to be found. I never did get his mobile nr or anything. So that's a dead end.
Well now I'm stuck, the trailer gate metal is just 1.6mm thick so I can't use my old arc welder, that would just blow the metal away. I need someone with a mig or tig welder willing to take a few dollars if I spin around with the box trailer. Anyone?
Trailer hinges job 2 mres.jpg
- Ian -
-
21st Jan 2017, 11:04 AM #2Mechanical Butcher
- Join Date
- Oct 2004
- Location
- Southern Highlands NSW
- Posts
- 1,898
If you don't have success welding to the sheet, may I suggest another approach?
I don't like those barrel style hinges on trailers. They are troublesome even when new and worse as they wear and get rusty.
As an alternative, I prefer to use some pieces of flat bar about 6x30, drill them for 10mm bolts, nyloc nuts & washers near the ends - there's your hinges.
These could be more easily welded to your steel angle frame.
I thought mine could wear out after a while, but many years later they're still good.
I'd take a photo, but someone's borrowed my trailer.
Jordan
-
21st Jan 2017, 02:01 PM #3China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
No reason why you can't weld 1.6mm with a arc welder, just use a series of short runs inked together I have done this on many occasions then if you want you can run a cover pass over the top.
-
21st Jan 2017, 09:28 PM #4Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
If you don't find a better option, I'd be happy to have a go at it in exchange for a 6-pack of a decent IPA.
Russell.
-
21st Jan 2017, 10:41 PM #5
-
21st Jan 2017, 11:18 PM #6
If Rusty can't do it i can MIG it. Im in Tuggers.
1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
22nd Jan 2017, 09:54 AM #7Diamond Member
- Join Date
- Jun 2010
- Location
- Canberra
- Posts
- 1,322
-
22nd Jan 2017, 11:31 AM #8
Pialligo's pretty good. I'm no expert on the ales either, but the California IPAs seem to get great reviews - but so many distinctive tastes and it all seems to come down to individual preference - maybe we could have a go with them and see what the fuss is all about. If no good, it'll make great snail bait. I'll send you a PM anyway.
Ueee, thanks too for offering a hand. Actually do you have a way to cut internal keyways? I've got a vertical milling head in bits here that I'm stuck on for want of 3/16" keyways on the replacement drive gears. Maybe I should PM you about that.
-
23rd Jan 2017, 12:16 AM #9
I am fairly sure i have a 3/16" broach. I may even have the correct sized bush! PM me with the details and i'll let you know if i can do it.
1915 17"x50" LeBlond heavy duty Lathe, 24" Queen city shaper, 1970's G Vernier FV.3.TO Universal Mill, 1958 Blohm HFS 6 surface grinder, 1942 Rivett 715 Lathe, 14"x40" Antrac Lathe, Startrite H225 Bandsaw, 1949 Hercus Camelback Drill press, 1947 Holbrook C10 Lathe.
-
23rd Jan 2017, 06:40 AM #10Philomath in training
- Join Date
- Oct 2011
- Location
- Norwood-ish, Adelaide
- Age
- 59
- Posts
- 6,561
Ewan, send me a PM if you haven't; I have and can send tools across if it helps.
Michael
Similar Threads
-
Magnabend hinges
By .RC. in forum METALWORK GENERALReplies: 25Last Post: 23rd Jun 2020, 10:23 AM -
Pivot hinges solution
By vicente in forum METALWORK GENERALReplies: 9Last Post: 16th Apr 2013, 11:08 AM -
welding trailer hubs
By welder in forum WELDINGReplies: 8Last Post: 28th Mar 2011, 07:46 PM -
Metal Hinges
By Jarrada in forum METALWORK GENERALReplies: 2Last Post: 15th Oct 2006, 12:42 PM