26th Dec 2016, 03:04 PM #1Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Oxygen pressure for brazing
Hi All,
Santa brought me a Cigweld Cutskill blowpipe, mixer and #8 brazing tip for Christmas to replace the old one in my oxy-LPG setup. I tried it out today, but I'm getting a pulsating flame. The regulator needle flickers in sync with the pulsing of the flame. I posted here about this a couple of years ago and the consensus was the reg was stuffed. However the problem went away if I used a cutting tip, which I often do to braze heavy pieces, so I didn't replace the reg at the time. I figured the reg didn't like working at low flow rates.
I've done a bit of research today and BOC recommend 50kPa fuel and oxy pressure for all their welding tips. On my oxy reg 50kPa is barely off the stop (see pic). Obviously this reg isn't optimal for my setup, so I went searching for a new oxy reg. However all oxy regs BOC sells allow very high oxygen pressures. For example: Cutskill Oxygen Regulator VI 800kPa – Cigweld
I don't use my oxy-LPG set for cutting. Do I need a regulator with a lower output pressure?
Cheers,
Chris
-
26th Dec 2016, 10:45 PM #2Most Valued Member
- Join Date
- Sep 2010
- Location
- Lebrina
- Posts
- 1,915
50 kPa is the textbook pressure to run for welding and brazing tips but higher pressures can be used, albeit at the expense of more touchy adjustments at the blowpipe valves. Your regulator definitely has issues, but you may find that increasing pressures to say 100 kPa for both oxy and lpg may alleviate your issues enough to get you out of trouble.
There may be special low pressure regs out there, but most just use the standard run of the mill ones like the cutskill one you found. Tesuco make reasonably priced regs and gas equipment too, so give them a look as well.
One final thought. You are using an Oxy LPG tip I assume?
-
27th Dec 2016, 09:19 AM #3Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Hi Karl,
Thanks for the reply.
This is what I'm finding. If I crank the reg pressure up, setting the oxy becomes very touchy. I have to very gingerly open the oxy valve at the blowpipe to prevent to LPG flame blowing out. It's always been a pain for me to light an oxy-LPG brazing tip, but higher pressure definitely makes it worse.
I found a BOC 8000 reg that only goes to 600kPa. That should be an improvement. I'll check out Tesuco.
https://www.boc.com.au/shop/en/au/bo...r-105105-p-112
Yes I am.
I found this on another website. If it's true it would explain the problem I'm having:
"Most regulators are notoriously inaccurate for pressure setting in the first 10-15% of their working range, and will pulsate or have pressure loss. The reason is that the spring that holds the diaphraphm in place doesn't have enough tension in the lower pressure settings. Most regulators won't become totally accurate until they are set at least at 25% of their working range."
Edit: I found this Tesuco reg. 150kPA out. Might do the trick. At $53 it's a lot cheaper than the BOC.
https://www.nationalwelding.com.au/r...n-type-10-in-2
-
27th Dec 2016, 02:34 PM #4Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Some progress. The reg stopped pulsing when I tried it today. Perhaps the diaphragm gets sticky if not used for a while?
I bought a size 15 tip today. The higher flow rate makes setting the oxy valve on the blowpipe a lot easier.
I've solved the difficult lighting issue. If I crack open the oxy tap I get a good light up. I'd always thought this was a no-no, but I saw a video by Harris which recommends this technique.
A lower pressure reg would still make setting the oxygen easier with the smaller tips.
-
27th Dec 2016, 04:25 PM #5China
- Join Date
- Dec 2005
- Location
- South Australia
- Posts
- 1,658
This might sound condescending but you are using a LPG regulator
-
27th Dec 2016, 05:03 PM #6Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Yes I am. It's a Cigweld adjustable gauge-less reg. I just crack it open, which gives plenty of gas. I should probably upgrade it to a reg with a gauge.
-
29th Dec 2016, 09:32 PM #7Member
- Join Date
- Nov 2015
- Location
- Brisbane Australia
- Posts
- 85
-
2nd Jan 2017, 10:01 PM #8Most Valued Member
- Join Date
- Nov 2007
- Location
- melbourne australia
- Posts
- 3,228
Chris
Similar Threads
-
Oxygen in mig gas
By meadow street in forum WELDINGReplies: 20Last Post: 16th Nov 2014, 12:12 AM -
Bernzomatic OX2500TK - Larger Oxygen Bottle + Gas / Oxygen Prices
By cmatten in forum WELDINGReplies: 4Last Post: 24th Jun 2014, 10:22 AM -
Oxygen Bottle buy/hire?
By rrjtedge in forum WELDINGReplies: 1Last Post: 2nd May 2011, 11:41 PM -
Anyone making their own oxygen at home??
By Mathuranatha in forum WELDINGReplies: 9Last Post: 17th Mar 2008, 05:40 PM -
Decanting Oxygen/ LPG --any problems?
By Mathuranatha in forum WELDINGReplies: 11Last Post: 15th Mar 2008, 11:31 AM