Good morning everyone.
I broke the mounting on the 60 years old scooter engine over the weekend. I am wondering if anyone could help to weld the piece back or knows any service in Melbourne I could get it fixed? I am on the eastern but willing to travel with it.
Your help or direction would be greatly appreciated. I'll remove the parts prior.
Thanks,
Trong
-
16th Feb 2015, 04:16 PM #2Member
- Join Date
- Jul 2012
- Location
- Malvern East
- Posts
- 84
You Broke it good mate
I hate to say it but Jesus that's smashed good
I can recommend Headwork's in Murrumbeena to do that repair BUT you are going to need to strip it to the bare cases to do it and either have Basil make a aliment dowel to suit it or you supply it
Good Luck Mate
Bruce
-
16th Feb 2015, 10:31 PM #3Golden Member
- Join Date
- Jun 2007
- Location
- Vic
- Age
- 48
- Posts
- 544
Thanks Bruce,
Yes almost heart broken after that, I couldnt sleep that night. Luckily I just found the case from ebay USA, postage is the killer but at least It will be the same again.
Regards,
Trong
-
17th Feb 2015, 12:35 PM #4Member
- Join Date
- Jul 2012
- Location
- Malvern East
- Posts
- 84
Lucky Find
Yes i know how heart breaking it can be, I'm used to doing a lot of case repairs on old trail bikes for vinduro etc so am used to the cost and repair side not a lot of people are mate lucky find on that spare case
Good Luck with it Bruce
Similar Threads
-
whats the easiest way to weld aluminium?
By bobsreturn2003 in forum WELDINGReplies: 13Last Post: 2nd Oct 2014, 01:55 AM -
How do I TIG Weld 1mm Aluminium
By Watts2759 in forum WELDINGReplies: 23Last Post: 23rd Aug 2011, 09:28 PM -
Black stuff oozing out of my alloy tig weld while welding.
By gozz in forum WELDINGReplies: 2Last Post: 26th May 2010, 11:55 PM