    Hi Guys im interested in makeing a few things out of aluminium checker plate in 2.5 mm thick, my question is what sort of welder u would recomend MIG or Tig, i have some experiance with mig on steel but none with tig and what make would u recomend at about the $1500 mark cheers

  2. #2
    Join Date
    Apr 2008
    Location
    Perth
    Posts
    269

    Default Welder

    Don't know where you live in oz bloke, but some forum members on here swear by TokenTools, check out their website, you will need a Tig that does AC/DC for alloy. Think TokenTools are in Wagga, or near abouts.

    DD

  3. #3
    Join Date
    May 2013
    Location
    Australia
    Posts
    4

    Default

    Tig is the go in that thickness range. When looking for a machine it must be acdc

  4. #4
    Join Date
    Sep 2010
    Location
    Lebrina
    Posts
    1,914

    Default

    Definitely TIG if you are restricted to only one welder.
    $1500 will definitely get you into something very workable along with a selection of consumables and an auto shield.
    In case you haven't already considered it, you will be needing a 15A power point to run your new toy.

  5. #5
    Join Date
    Sep 2014
    Location
    australia
    Posts
    9

    Default

    thanks guys tig it is will let u know how i go

  6. #6
    Join Date
    Aug 2009
    Location
    Sydney, NSW, Australia
    Posts
    1,841

    Default

    i would go with a MIG spool gun 2.5mm will be a piece of cake to weld, i welded 1.6mm with a cheap ebay MIG/spool gun on youtube done it very easy but the slightest gap between the two pieces being welded will blow a hole

    i bought the LOTOS mig from ebay for $450 as a buy now price brand new came with a regulator and spool gun (compatible with lincoln) the seller list about 2 LOTOS MIG/spool gun welders a month on ebay

    ive just uploaded 2 pictures of my 1.6mm spool gun welds and im only very basic welder just learning to weld

    i spent over $600 on a TIG machine and it was nothing but a pain in the ass to use i never got the hang of it eventually selling it and loosing out on money i bought this welder

    here is a video doing that 1.6mm aluminum weld so u can see it actually being welded

    https://www.youtube.com/watch?v=KJnM...lOHw65q9PUliCw
    Attached Images Attached Images

  7. #7
    Join Date
    Dec 2014
    Location
    NA
    Posts
    2

    Default You can select one of the following machines:


Similar Threads

  1. QUEENSLAND Cig welder transarc tradesman HD (stick/arc welder) 3phase
    By dkaoffroad in forum METALWORK - Machinery, Equipment, MARKET
    Replies: 0
    Last Post: 8th Jun 2013, 10:45 AM
  2. Bob the Welder
    By Charleville in forum WELDING
    Replies: 1
    Last Post: 1st Jul 2008, 07:33 AM
  3. What do you think of this welder?
    By jackaroo in forum METALWORK GENERAL
    Replies: 9
    Last Post: 7th Jul 2007, 01:48 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •