    have seen this at several shows, the bloke soldered aluminium coke cans with it. I bought some but never used it.
    Kryn

  3. #3
    Join Date
    Jun 2010
    Location
    Canberra
    Posts
    1,322

    Default

    Yeah, I've seen these at field days for years, and have used them on the odd occasion with reasonable results. However, for the ones I have, you need to have a dedicated stainless steel brush for cleaning the joint before you braze. The ones linked to above don't seem to require this, and claim to be flux-cored, so perhaps they're different?

  4. #4
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,656

    Default

    As said above similar rods have been around for years, I have used them on various jobs secret is extreme clealiness and don't overheat, can't see why you would destroy the hose by cutting the tails off you only need to split the crimps

  5. #5
    Join Date
    Jan 2007
    Location
    Katoomba NSW
    Posts
    209

    Default

    I have these. They work great. Have welded up a few Ali things and I am not a welder by any stretch of the imagination.
    Built: a Bench,a Desk,an Archery Display,

    Those were the droids I was looking for.

  6. #6
    Join Date
    Jun 2013
    Location
    Brisbane
    Posts
    4

    Default Aluminium Brazing

    Hi Guys,

    My name is Mick from brazelikeapro.com. If you need any help with aluminium brazing, I would be glad to help.

  7. #7
    Join Date
    Jun 2010
    Location
    Canberra
    Posts
    1,322

    Default

    Quote Originally Posted by Brazelikeapro View Post
    Hi Guys,

    My name is Mick from brazelikeapro.com. If you need any help with aluminium brazing, I would be glad to help.
    Well howdy there, Mick.

    First up, are your brazing rods any different from the ones we see at field days with the guy welding up soft-drink cans? I ask this because that system puts a great deal of emphasis on using a clean, dedicated stainless-steel brush to prep the joint, where with your system, not so much.

  8. #8
    Join Date
    Jun 2013
    Location
    Brisbane
    Posts
    4

    Default Brazing Rods

    Quote Originally Posted by RustyArc View Post
    Well howdy there, Mick.

    First up, are your brazing rods any different from the ones we see at field days with the guy welding up soft-drink cans? I ask this because that system puts a great deal of emphasis on using a clean, dedicated stainless-steel brush to prep the joint, where with your system, not so much.
    Hi RustyArc,

    Our rods are not the same as you see at the shows. Our rods are specially designed for brazing Automotive A/C components. They are a flux core rod and about 1.5mm thick. We don't have to clean parts with a SS wire brush. we do recommend all components are free of any oils.

  9. #9
    Join Date
    Jun 2013
    Location
    Brisbane
    Posts
    4

    Default

    Quote Originally Posted by China View Post
    As said above similar rods have been around for years, I have used them on various jobs secret is extreme clealiness and don't overheat, can't see why you would destroy the hose by cutting the tails off you only need to split the crimps
    Hi China,

    The reason you should cut the tail off and braze a new tail on is because when you crimp a ferrule onto a tail, you get tail collapse. This means the tail is crushed in the middle and may not form a correct seal. This happens more on aluminium tails.

  10. #10
    Join Date
    Jun 2013
    Location
    Brisbane
    Posts
    4

    Default Aluminium Brazing

    Quote Originally Posted by eskimo View Post
    Hi Eskimo,

    These rods are designed for brazing Automotive A/C components. I am happy to help you with your questions, if you need help.

Similar Threads

  1. Aluminium brazing
    By kenny_10 in forum WELDING
    Replies: 1
    Last Post: 1st Nov 2011, 12:56 PM
  2. Brazing aluminium to metal
    By Tiger in forum WELDING
    Replies: 11
    Last Post: 28th Jul 2009, 08:00 PM
  3. Brazing
    By garym in forum METALWORK GENERAL
    Replies: 34
    Last Post: 9th Aug 2007, 12:12 AM
  4. Help with brazing with MAP
    By BobL in forum METALWORK GENERAL
    Replies: 2
    Last Post: 5th Nov 2006, 03:28 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •