Gas volume calculator
Hey,
I'm trying to work out the volume in liters of a Air Liquide Dx size Argon bottle. They are 2.2 cubic meters at ~16000 kPa. Is that 2200 liters?
I'm trying to figure out long a bottle will last at typical TIG flow rates. Can anyone throw me a bone?
Cheers
-
18th Feb 2013, 05:24 PM #2Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
Hi, that sounds about right.
Kryn
-
18th Feb 2013, 07:07 PM #3Member
- Join Date
- Jul 2008
- Location
- Lismore, NSW
- Posts
- 54
Thanks man. I could expect about 5 hours from this size bottle?
-
18th Feb 2013, 07:28 PM #4New Member
- Join Date
- Jan 2013
- Location
- Blue Mountains
- Posts
- 4
Gas volume calculator
Quote I've always been told thickness of wire x10. So 0.8mm wire = 8l gas/min, 0.6 = 6l/min etc. - which seem s to work well enough. Unquote
Link http://www.mig-welding.co.uk/forum/s...ad.php?t=32882Wood burns faster when you have to cut and chop it yourself.
~ Harrison Ford
-
18th Feb 2013, 07:45 PM #5Golden Member
- Join Date
- Feb 2010
- Location
- Ballina, NSW
- Posts
- 900
Yep 2.2m3 = 2,200 litres.
TIG welding will typically use between 6 and 12 lpm depending on cup size, how sensitive the metal is, etc. I typically use 8 lpm, that that means your cylinder would last me 2,200/8 = 275 minutes, or about 4.5 hours. When you factor in pre/post flow, gas purge or any other use, you might only have 3 to 4 hours of actual arc time.
-
19th Feb 2013, 05:33 AM #6Member
- Join Date
- Jul 2008
- Location
- Lismore, NSW
- Posts
- 54
Thanks again fellas. I thought my math skills weren't too shabby.
-
19th Feb 2013, 01:03 PM #7Most Valued Member
- Join Date
- May 2011
- Location
- Murray Bridge S Aust.
- Age
- 71
- Posts
- 5,942
-
20th Feb 2013, 02:35 AM #8Intermediate Member
- Join Date
- Jul 2011
- Location
- Mackay
- Posts
- 37
-
3rd Apr 2013, 03:45 PM #9Senior Member
- Join Date
- Mar 2011
- Location
- Taree NSW
- Posts
- 119
l/m or p.s.i.?
Does anyone have any experience with the Air liquide mini top oxy/acetylene cylinders? - when I went to tech we were taught to use (from memory) 5 p.s.i. of acetylene and 14 p.s.i. of oxy when welding panel steel -the regulators on the Minitops are apparently graduated in litres/min. and they have no delivery pressure gauge - Air liquide at this stage haven't been very helpful so can anyone advise me how to set my regulators in l/m to weld panel steel?