Hi Blokes
I retired my 30yr old CIG Transarc 140amp EasyWelder yesterday and bought a new Lincoln Inverter welder. Wanted to see what all the fuss was about using a inverter over and old buzzbox.
Sure is a big difference, apart from being quite when welding, the amps settings are totally different to the old machine, the welds look clean and full, and it only weighs 7.5 kilos. No more using the Kevrek crane on the back of my ute to pick up the old girl (welder).
DD
-
17th Aug 2012, 03:27 AM #2
As much as I love my couple of inverter welders, There is still s place for your old 140amp AC machine.. Some electrodes dont like DC inverters.
All I am saying is dont get rid of the old girl.
Matt
Sent from my GT-S6102 using Tapatalk 2Warning Disclaimer
-
19th Aug 2012, 08:05 PM #3Novice
- Join Date
- Aug 2012
- Location
- Taree
- Posts
- 20
Sounds like you are doing much better than me. I bought a new inverter unimig 170 arc welder and I hate it. I find it much more difficult to weld with than my fathers old ac monarc 130 amp arc welder. The electrodes stick more and is difficult to maintain a stable arc. Admittedly I'm a beginner stick welder.
-
20th Aug 2012, 10:35 AM #4Senior Member
- Join Date
- Apr 2008
- Location
- Perth
- Posts
- 269
Sticking
BP
Must admit I found the same problem. The welding rods are old, SatinCraft13 in various sizes, I touched up a heap of the ends on the linisher, remember my bro-in-law telling me way back that to strike a good arc is to ensure the end is cleaned up, he use to rub the end onto whatever was at hand before he placed that in the holder.
The dragon does not like bits of blue on her nice concrete, so I did them on the linisher. Wish I could get some more of them Strata 555 rods, for me they were cream to weld with.
DD
Similar Threads
-
What welder
By stevo81 in forum WELDINGReplies: 6Last Post: 15th Jun 2011, 03:50 PM -
Bob the Welder
By Charleville in forum WELDINGReplies: 1Last Post: 1st Jul 2008, 07:33 AM -
First Welder
By westcoast in forum WELDINGReplies: 13Last Post: 19th Jan 2008, 10:25 AM -
TIG welder
By gpigeon in forum METALWORK GENERALReplies: 9Last Post: 11th Jun 2007, 10:27 PM -
MIG Welder DOA :(
By Dean in forum WELDINGReplies: 12Last Post: 4th Jun 2007, 10:29 PM