    Default welding thin material with stick inverter

    G,day , need to weld something very thin with my stick [inverter] . will use 1.6 rods at 40 amps or a bit less ,just cant remember which way around the leads should be connected to reduce blowing holes . I think its rod -ve but not sure . [hardly weld much thin stuff with stick but its stainless so cant use oxy or braze it]
    Thanks fellers . ---- mat ---

  2. #2
    Join Date
    Feb 2010
    Location
    Ballina, NSW
    Posts
    900

    Default

    Hi Mat,

    I'd use DCEP (hand piece +ve) as I think you get a more controllable arc, but honestly I don't think it makes a heap of difference despite all the various theories out there. See this thread http://www.woodworkforums.com/f160/p...larity-144808/ - my conclusion is that with stick, any heat that is concentrated on the electrode is transferred to the work anyway (via droplets of molten metal), so polarity is less important than it is with a non-consumable electrode (i.e. TIG welding). This makes sense theoretically and has proven to be the case in practice as well (at least for me).

    Oh yeah... check the manufacturers recommended polarity for your particular rods.

    One thing that is worth experimenting with is using slightly larger electrodes (2.4mm) - this can sometimes help with thin metal. What do you mean by "thin" anyway? - I'm talking about stuff like 1.2mm gal.

    Cheers

    - Mick

  3. #3
    Join Date
    Dec 2005
    Location
    South Australia
    Posts
    1,657

    Default

    No reason not to weld or braze it with oxy I have done it plenty of times

  4. #4
    Join Date
    Jan 2008
    Location
    Murwillumbah Nthn NSW
    Age
    68
    Posts
    118

    Default

    Quote Originally Posted by China View Post
    No reason not to weld or braze it with oxy I have done it plenty of times
    well its muffler grade stainless , I've never had much luck brazing stainless before , any hints ? thanks -- mat --

  5. #5
    Join Date
    Sep 2007
    Location
    Country West Oz
    Age
    77
    Posts
    169

    Default

    I weld a hell of lot of thin walled tube (exhaust pipe) with an inverter welder.
    I use 2.4mm rods and it took me quite while to master the tecnique. I have tried the 1.6mm rods and can't seem to do any good with them.
    However this is not stainless so I'm not sure how you go there
    Regards
    Bradford

  6. #6
    Join Date
    Jan 2008
    Location
    Murwillumbah Nthn NSW
    Age
    68
    Posts
    118

    Default

    the 1.6 rods did it . looks like the muffler from hell , but no bubbles from the welds when submerged in the dam [on the third attempt] . So there ya go a thin stainless muffler [looks less than half a mm] can be welled with a stick welder if you dont mind spending more time filling the holes you blow than fixing the original cracks .

Similar Threads

  1. problem TIG butt welding thin material
    By Brendon5374 in forum WELDING
    Replies: 17
    Last Post: 15th Sep 2011, 08:51 AM
  2. Inverter stick comparisons
    By Grahame Collins in forum WELDING
    Replies: 54
    Last Post: 25th Feb 2011, 09:46 PM
  3. BOC Smootharc 130 Inverter Stick/TIG
    By distractor in forum WELDING
    Replies: 3
    Last Post: 25th May 2010, 11:42 PM
  4. Stick Inverter observations
    By scanfor in forum WELDING
    Replies: 11
    Last Post: 25th Feb 2010, 09:37 PM
  5. Inverter Arc / Stick welder recommendations
    By Matty5700 in forum WELDING
    Replies: 10
    Last Post: 17th May 2009, 10:53 AM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •